Welding tsvimbo AWS A5.1 E6013 (J421)

Tsanangudzo Pfupi:

Welding rods AWS A5.1 E6013 (J421) yakakodzera welding yepasi kabhoni simbi chimiro, kunyanya kune yakatetepa ndiro simbi ine pfupi discountinuous weld uye chinodiwa yakatsetseka welding pass.


Product Detail

Product Tags

Welding rods AWS A5.1 E6013 (J421) yakakodzera welding yepasi kabhoni simbi chimiro, kunyanya kune yakatetepa ndiro simbi ine pfupi discountinuous weld uye chinodiwa yakatsetseka welding pass.

Zvikamu:

ISO 2560-A-E35 0 RA 12

AWS A5.1: E6013

GB/T 5117 E4313

Hunhu:

AWS A5.1 E6013 (J421) ari rutile mhando electrode.Inogona kuve welding zvese AC & DC magetsi sosi uye inogona kuve yeese chinzvimbo.Iyo ine yakanakisa welding performance seyakagadzika arc, spatter shoma, nyore kubviswa slag uye kutonga-kugona etc. Rutile-cellulosic electrode ine yakanaka weld kugona munzvimbo dzese kusanganisira vertical pasi.Yakanakisa gap-bridging uye arc-inorova kugona.Kune tack welding uye load fit ups.General chinangwa cheindasitiri nekutengeserana, gungano uye chitoro welding.

Chenjerera:

Kazhinji, haufanire kuomesa zvakare erekitirodhi usati welding.Kana ichinge yakanganiswa nekunyorova, inofanira kuomeswa zvakare pa150 ℃-170 ℃ kwe 0.5-1 awa.

Welding Position:

PA, PB, PC, PD, PE, PF

AWS A5.1 E6013 inokodzera welding zvimiro zvakagadzirwa ne low kabhoni simbi, inoita zvakanaka kwazvo mukukwesha mahwendefa matete uye madiki saizi simbi uye zvakare ine kuita kwakanaka kwazvo mumamiriro ezvinhu anoda kunaka uye kwakachena bead kutaridzika.

Kemikari Kuumbwa kweAll Weld Metal: (%)

Kuumbwa Kwemakemikari

C

Mn

Si

S

P

Ni

Cr

Mo

V

Zvinodiwa

≤0.10

0.32-0.55

≤0.30

≤0.030

≤0.035

≤0.30

≤0.20

≤0.30

≤0.08

Typical Results

0.08

0.37

0.18

0.020

0.025

0.030

0.035

0.005

0.004

Mechanical Properties yeDeposited Metal

Test Item

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) 0℃

Zvinodiwa

440-560

≥355

≥22

≥47

Typical Results

500

430

27

80

Reference Current (DC)

Diameter

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

40 ~ 70

50 ~ 90

80 ~ 130

150 ~ 210

180 ~ 240