AWS: SFA 5.4 E318-16 Stainless Steel Welding Electrodes, Best Welding Rods

Tsanangudzo Pfupi

A212 (AWS E318-16) is a low-carbon Cr18Ni12MoNb Stainless steel electrode ine niobium-containing stabilizer ine titanium-calcium coating.


Product Detail

Product Tags

Stainless Simbi Welding Electrode

A212

GB/T E318-16

AWS A5.4 E318-16

Tsanangudzo: A212 i-low-carbon Cr18Ni12MoNb Stainless steel electrode ine niobium-containing stabilizer ine titanium-calcium coating.Inogona kushandiswa kune ese AC uye DC ine yakanakisa mashandiro ekushanda.Simbi yakaiswa ine zvirinani intergranular corrosion performance pane A202 uye A207.

Chikumbiro: Inoshandiswa pakushongedza yakakosha 06Cr17Ni12Mo2, Ultra-yakaderera kabhoni Cr17Ni14Mo2 uye zvimwe zvimiro zvesimbi zvisina tsvina, senge urea synthesis tower, vinylon zvishandiso uye zvimwe zvikamu zvakafumurwa kune yakasimba corrosive media.

 

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Nb

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

6 XC ~ 1.00

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥550

≥25

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Cherechedza:

1. Iyo electrode inofanira kubikwa kweawa imwe panguva inenge 150 ℃ isati yaitwa welding;

2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanira kushandiswa zvakanyanya sezvinobvira kuti ipinde zvakadzama.uye ikozvino haifaniri kunge yakakura zvakanyanya kudzivirira kutsvuka kwetsvimbo yewelding;

3. Kurwisana kwekuora kwesimbi yakaiswa kunotsanangurwa nechibvumirano chechipiri chekugovera uye kudiwa.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 

 


  • Zvakapfuura:
  • Zvinotevera: