Nickel Alloy Welding Wire ERNiCrMo-3 Tig Wire

Tsanangudzo Pfupi

ERNiCrMo-3 ndeye yakakwira nickel alloy waya yakagadziridzwa yewelding uye cladding nickel-based alloys akadai 625 kana zvimwe zvakafanana.


Product Detail

Product Tags

Nickel AlloyWelding WireTig WireERNiCrMo-3

 

Features uye Applications

Highnickelalloy wire yakagadziridzwa welding uye claddingnickel-based alloys akadai se625 kana zvimwe zvakafanana.

Solid yakadhonzwa nenzira yakasarudzika yekuwana yakachena uye yemhando yepamusoro welds ine inopenya seam uye yakanakisa ductility.

Iyo weld simbi ine yakanaka kwazvo ma mechanical properties pakakwirira uye yakaderera tembiricha.

Kuramba kwakanaka kugomba uye kusagadzikana ngura.

Tembiricha yekushanda inokurudzirwa inotangira pa cryogenic kusvika pa540°C.

Inowanzo shandiswa muindasitiri yemakemikari process, marine engineering, nuclear reactor components, aerospace uye mukati memidziyo yekudzora kusvibiswa nezvimwe.

Typical Base Materials

Inconel 601, Incoloy 800, Alloy 625, Alloy 825, Alloy 926*
* Runyoro rune mufananidzo, kwete ruzere

 

Mitemo
EN ISO 18274 - Ni 6625 - NiCr22Mo9Nb
AWS A5.14 – ER NiCrMo-3

 

Kuumbwa Kwemakemikari%

C%

Mn%

Fe%

P%

S%

Si%

Cu%

max

max

max

max

max

max

max

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ni%

Co%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

max

max

max

20.00

3.15

8.00

min

1.0

0.40

0.40

23.00

4.15

10.00

 

Mechanical Properties
Tensile Simba ≥760 MPa  
Goho Simba ≥415 MPa  
Elongation ≥35%  
Impact Simba ≥100 J  

Mechanical zvivakwa zvine fungidziro uye zvinogona kusiyana zvichienderana nekupisa, kudzivirira gasi, welding paramita uye zvimwe zvinhu.

 

Kudzivirira Magasi

TS EN ISO 14175 TIG: I1 (Argon)

 

Welding Positions

TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Packaging Data
Diameter Urefu Kurema  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

 

 

Mhosva: Kunyange zvese zvine musoro zvaitwa kuti ive nechokwadi chechokwadi cheruzivo rwurimo, ruzivo urwu runogona kuchinja pasina chiziviso uye rinogona kungoonekwa serinokodzera kutungamira.

 