Waya yeAWS A5.22 E312T-1 FLUX-CORED

Kuumbwa kweMakemikari

Fe C Cr Ni Mo Mn Si P S N Cu
Kuenzana 0.15 28.0-32.0 8.0-10.5 0.5 0.5-2.5 1.0 0.04 0.03 — 0.5

Kukosha kumwe chete ndiko kwakanyanya kunze kwekunge zvataurwa neimwe nzira.

Tsananguro uye Mashandisirwo
E312T-1 iwaya yesimbi isina tsvina yerudzi rweAISI 312 ine flux-core ine hunhu hwakanaka hwekushanda. Inogadzira madhipoziti akaomarara, ane simba guru rekudhonza kupfuura chero simbi dzisina tsvina dze austenitic. Madhipoziti e weld anoenderana nehunhu uye hunhu hwemakanika esimbi yebase yeAISI 312. Madhipoziti e weld angangoita 23 Rockwell C sezvaanoshandiswa. Kugadzira muchina kunofanirwa kuitwa nekunonoka kwekudya sezvo madhipoziti e weld anodzivirira kupisa, ngura uye kupfeka. Chimiro chesimbi chakasiyana ndeche ferrite yakasungirirwa mu austenite matrix. Izvi zvinoita kuti madhipoziti acho arambe kupwanyika zvakanyanya.
Inoshandiswa kusanganisa simbi dzepasi dzine ongororo yakafanana pamwe chete nesimbi dzakasiyana. Inweld E312T-1 inoshanda zvakanaka pasimbi dzinodzivirira kukweshana, simbi dzemanganese, simbi dzinoomesa, simbi dzechitubu, plate yezvombo, simbi dzinobereka zvakawanda uye yekubatanidza simbi dzinopisa zvakanyanya kusimbi dzekabhoni nesimbi dzisina alloy yakawanda. Sarudzo yakanaka sechikamu chepasi (buffer layer) chesimbi dzakaoma.
Zvivakwa zveSimbi Zvakajairwa Zvekunamira
Simba reKudhonza reAWS Spec: 95,000 psi Simba reKuburitsa: 75,000 psi
Kureba: 35%

Zvinokurudzirwa
FCAW (DCEP – Electrode +) 100% CO2 kana 75% – 95% Ar / Balance CO2

 

Dhayamita yewaya Voltage Amperage
0.045” 25-30 130-180
1/16” 24-29 160-250

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave tichiita basa rekugadzira ma electrodes ekuwelda,tsvimbo dzekunamira, uye zvinoshandiswa pakusonwa kwemidziyo kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira maelectrode esimbi isina ngura, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni & cobalt, mawaya esimbi yekabhoni & low alloy, waya dzesimbi yekabhoni & low alloy, waya dzesimbi yekabhoni, waya dzesimbi yekabhoni, waya dzakavharirwa negesi, waya dzesimbi yekabhoni ...


  • Yakapfuura:
  • Zvinotevera: