E71T-1C/1M-PLUS A5.20, Carbon Steel Flux Cord Arc Welding Electrodes Mig Welding Wire

Tsanangudzo Pfupi

E71T-GS isimbi yekabhoni, flux-cored electrode yekushandisa pasina kunze kwekudzivirira gasi.Iri electrode rakagadzirirwa welding thin-gauge carbon steel, kubva pa3/16” kusvika pa22 geji.


Product Detail

Product Tags

E71T-GS isimbi yekabhoni, flux-cored electrode yekushandisa pasina kunze kwekudzivirira gasi.Iri electrode rakagadzirirwa welding thin-gauge carbon steel, kubva pa3/16” kusvika pa22 geji.

Typical Applications: single-pass weldments;chigadzirwa ichi chakagadzirirwa weld chaizvo zvinobudirira pamusoro pemarara zvinhu uye chinogona kushandiswa pane mamwe maaluminium akafukidzwa zvakare.E71T-GS haidi yekunze gasi-kudzivirira uye inofanira kunge yakasungwa neDCEN (yakatwasuka polarity).

AWS Kirasi: E71T-GS Certification: AWS A5.20/A5.20M:2005
Alloy: E71T-GS AWS/ASME SFA A5.20

 

Welding Position:
H, F, V, O
Zvazvino:
DCEN
Yakarurama Polarity

 

Transverse Tensile Simba, kpsi: 86.4min (Base simbi kutsemuka)
Inotungamirirwa Bend Test Inosangana neAWS zvinodiwa

 

Typical Wire Parameters
Diameter Process Amps Volts Wire Feed Speed
in (mm)
.030″ 0.8 FCAW 50 15 80
    FCAW 100 16 225
    FCAW 150 17 375
    FCAW 175 17 445
.035″ 0.9 FCAW 75 15 70
    FCAW 100 16 110
    FCAW 150 17 180
    FCAW 200 18 305
.045″ 1.2 FCAW 100 15 70
    FCAW 150 16 120
    FCAW 200 17 195
    FCAW 225 17 245
1/6" 1.6 FCAW 150 17 60
    FCAW 200 18 85
    FCAW 250 18 135
    FCAW 300 19 180
5/64” .078 FCAW 200 19 60
    FCAW 250 20 80
    FCAW 300 21 115
    FCAW 325 120 6.6

Wenzhou Tianyu Electronic Co., Ltd yakavambwa muna 2000.welding tsvimbo, uye welding consumables kweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.