E2553T1-1/4 AP Stainless Steel Flux Cord Welding Wire

Tsanangudzo Pfupi

E2553T1-4 AP flux-cored waya inoshandiswa kubatanidza duplex Stainless simbi alloys inosvika 25% Chromium.


Product Detail

Product Tags

E2553T1-1/4 AP FLUX-CORED WAYA

CLASSIFICATION
AWS 5.22 Kirasi E2553T1-1 uye E2553T1-4 / ASME SFA 5.22 Kirasi E2553T1-1 uye E2553T1-4
UNS# W39533 A#8 F#6

DESCRIPTION
E2553T1-4 ndeyese-chinzvimbo flux-cored waya yakagadzirirwa kumhanya pa75% Ar / 25% CO2.
Waya iyi yakagadzirirwa kuve neyakanakisa kubviswa kwe slag uye inomhanya ine spatter-isina globular kutamiswa.

APPLICATIONS
E2553T1-4 AP flux-cored waya inoshandiswa kubatanidza duplex Stainless simbi alloys inosvika 25% Chromium.
Aya duplex Stainless simbi alloys anosanganisa yakakwira tensile uye goho simba nekuvandudzwa kwekudzivirira kugomba, ngura, uye kusagadzikana ngura kuparuka.Izvi zvinodikanwa zvinowanzowanikwa mumakungwa, makemikari, uye petroleum maindasitiri.
Kana post-weld annealing ichidikanwa, iyi weld metal inoda tembiricha yepamusoro kupfuura inodiwa ne duplex base metal.

PROCEDURE
Hapana preheat.Tembiricha yepamusoro yepakati pe 300°F.
Annealing inogona kudikanwa kuti uwane yunifomu kuomarara pane akawanda-pass weldments.
Kupisa kunofanira kugumira ku5-40 KJ/IN.

TYPICAL CHEMISTRY

C Cr Ni Mo Mn Si P S N Cu
0.02 25.3 9.8 3.37 0.80 0.70 0.03 0.015 0.14 1.87

TYPICAL MECHANICAL PROPERTIES

HARDNESS 25 RC as welded 35 RC basa rakaoma
TENSILE SIMBA 110,000 PSI Min.
ELONGATION 15% Min.

WELDING PARAMETERS

SIZE VOLTAGE AMPERAGE GAS
.045" 25-30 130-220 75% Ar / 25% CO2 kana 100% CO2

 

Wenzhou Tianyu Electronic Co., Ltd yakavambwa muna 2000.welding tsvimbo, uye welding consumables kweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.


  • Zvakapfuura:
  • Zvinotevera: