Nickel Alloy Welding Wire ERNi-1 Nickel Tig Wire Filler Metal

Tsanangudzo Pfupi

ER-Ni1 inoshandiswa kugadzira uye kupfekedza Nickel 200 uye Nickel 201 alloys.


Product Detail

Product Tags

Nickel AlloyWelding WireTig WireERNi-1

Mitemo
EN ISO 18274 - Ni 2061 - NiTi3
AWS A5.14 – ER Ni-1

 

Features uye Applications

ER-Ni1 inoshandiswa kugadzira uye kupfekedza Nickel 200 uye Nickel 201 alloys.

Yakakwana yekubatanidza Monel alloys uye mhangura-nickelalloys kune carbon steels.

Ni1 ine yakakwana titanium yekudzora weld-simbi porosity pane welding maitiro.

Inowanzo shandiswa mumaindasitiri ekugadzira makemikari, synthetic fiber kugadzira & chikafu chekugadzira chikafu nezvimwe.

 

Typical Base Materials

Nickel 200 uye 201*
* Runyoro rune mufananidzo, kwete ruzere

 

Kuumbwa Kwemakemikari%
C% Mn% Fe% P% S% Si%  
max max max max max max  
0.05 0.80 0.70 0.030 0.010 0.75  
             
Cu% Ni% Co% Ti% Al%    
max 93.00 max 2.00 max    
0.20 min 1.00 3.50 1.00    

 

Mechanical Properties
Tensile Simba ≥410 MPa  
Goho Simba ≥200 MPa  
Elongation ≥30 %  
Impact Simba ≥100 J  

Mechanical zvivakwa zvine fungidziro uye zvinogona kusiyana zvichienderana nekupisa, kudzivirira gasi, welding paramita uye zvimwe zvinhu.

 

Kudzivirira Magasi

TS EN ISO 14175 TIG: I1 (Argon)

 

Welding Positions

TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Packaging Data
Diameter Urefu Kurema  
1.60 mm

2.40 mm

1000 mm

1000 mm

5 Kg

5 Kg

 

 

Mhosva: Kunyange zvese zvine musoro zvaitwa kuti ive nechokwadi chechokwadi cheruzivo rwurimo, ruzivo urwu runogona kuchinja pasina chiziviso uye rinogona kungoonekwa serinokodzera kutungamira.