AWS A5.4 E316L-16 Stainless Steel Welding tsvimbo Akanakisisa Welding Zvishandiso

Tsanangudzo Pfupi

A022 (AWS A5.4 E316L-16) is an ultra-low carbon Cr18Ni12Mo2 Stainless steel electrode ine titanium calcium coating.


Product Detail

Product Tags

Stainless Simbi Welding Electrode

A022                                                 

GB/T E316L-16

AWS E316L-16

Tsanangudzo: A022 is an ultra-low carbon Cr18Ni12Mo2 Stainless steel electrode ine titanium calcium coating.Inogona kushandiswa kune ese AC uye DC ine yakanaka maitiro ekuita.Iyo kabhoni yemukati yesimbi yakaiswa ndeye ≤0.04%, iyo inopa iyo yakanaka yekupisa kupisa, kusaita ngura uye kutsemuka kuramba.

 Chikumbiro: Inoshandiswa pakushongedza urea, synthetic fiber nemimwe michina uye yakafanana mhando yesimbi isina tsvina chimiro.Inogona zvakare kushandiswa chromium Stainless simbi, composite simbi uye dissimilar simbi isingakwanise kupisa kurapwa mushure mewelding.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥490

≥30

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Cherechedza:

1. Iyo electrode inofanira kubikwa kweawa imwe panguva inenge 150 ℃ isati yaitwa welding;

2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanira kushandiswa zvakanyanya sezvinobvira kuti ipinde zvakadzama.uye ikozvino haifaniri kunge yakakura zvakanyanya kudzivirira kutsvuka kwetsvimbo yewelding;

3.Kurwisana kwekuora kwesimbi yakaiswa kunotsanangurwa nechibvumirano chechipiri chekugovera uye kudiwa.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 


  • Zvakapfuura:
  • Zvinotevera: