AWS E312-16 Stainless Steel Welding Electrodes, Manual Metal Arc Electrodes, Solder

Tsanangudzo Pfupi

AFE312-16 (AWS E312-16) iCr29Ni9 duplex stainless steel electrode ine titanium-calcium coating.


Product Detail

Product Tags

Stainless Simbi Welding Electrode

AF312-16

GB/T E312-16

AWS A5.4 E312-16

Tsanangudzo: AFE312-16 iCr29Ni9 duplex Stainless steel electrode ine titanium-calcium coating.Inogona kushandiswa kune zvese AC uye DC ine yakanakisa kushanda kushanda.Nekuti ine molybdenum uye nitrogen, uye kabhoni yemukati yakadzikira zvakanyanya, simbi yakaiswa ine yakanaka kutsemuka uye kusaita ngura, kunyanya kushushikana kwekuora.

Chikumbiro: Inoshandiswa kugadzirwa kwe29-9 series simbi isina tsvina, simbi yakakandwa uye dissimilar simbi, uyewo welding yezvinhu zvinogara zvichitsemuka uye porosity.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.15

0.5 ~ 2.5

≤0.90

28.0 ~ 32.0

8.0 ~ 10.5

≤0.75

≤0.75

≤0.030

≤0.040

 

 

Mechanical zvimiro zve weld simbi:

Test chinhu

 Kusimba simba

Mpa

Elongation

%

Guaranteed

≥660

≥22

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~80

80 ~ 110

100 ~ 150

140 ~ 180

 

Cherechedza:

1. Iyo electrode inofanira kubikwa kweawa imwe panguva inenge 250 ℃ isati yaitwa welding.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 