AWS: SFA 5.4 E316-16 Stainless Steel Welding Electrodes

Tsanangudzo Pfupi

A201(AWS E316-16) isimbi yakaderera-kabhoni Cr18Ni12Mo2 isimbi isina tsvina electrode ine titanium-calcium coating.


Product Detail

Product Tags

Stainless Simbi Welding Electrode

A201                                      

GB/T E316-16

AWS E316-16

Tsanangudzo: A201 ndeye yakaderera-kabhoni Cr18Ni12Mo2 Stainless simbi electrode ine titanium-calcium coating.Inogona kushandiswa kune ese AC uye DC ine yakanakisa mashandiro ekushanda, kunyanya yakakodzera kune flat welding uye fillet welding yemahwendefa matete.Iyo yekupfekedza haishanduki yakatsvuka kana kuputika panguva yewelding.Nekuda kwekuwedzera kwe molybdenum kune simbi yakaiswa, ine yakanaka corrosion resistance, heat resistance uye crack resistance, kunyanya yekuramba chloride ion pitting corrosion.

Chikumbiro: Inoshandiswa kukwenenzvera 06Cr17Ni12Mo2 Stainless simbi zvimiro zvinoshanda muorganic uye inorganic asidhi (isina-oxidizing acid) yepakati, uye inogona zvakare kushandiswa kugadzira yakakwira chromium simbi kana dissimilar simbi isingagoni kupisa kupisa mushure mekunama.

 

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥520

≥30

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Cherechedza:

1. Elekitirodhi inofanira kubikwa kweawa imwe panguva inenge 250 ℃ isati yaitwa welding.Usabika kakawanda;

2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanira kushandiswa zvakanyanya sezvinobvira kuti ipinde zvakadzama.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.


  • Zvakapfuura:
  • Zvinotevera: