AWS: SFA 5.4 E308-16 Stainless Steel Welding Electrode

Tsanangudzo Pfupi

A102 (AWS E308-16) i-low-carbon Cr19Ni10 Stainless steel electrode ine titanium-calcium coating.


Product Detail

Product Tags

Stainless Simbi Welding Electrode

A102                                        

GB/T E308-16

AWS E308-16

Tsanangudzo: A102 i-low-carbon Cr19Ni10 Stainless steel electrode ine titanium-calcium coating.Inogona kushandiswa kune ese ari maviri AC uye DC uye ine yakanaka yekushandisa kuita.Iyo simbi yakaiswa ine yakanaka mechanical zvivakwa uye kuramba kune intergranular corrosion.

Chishandiso: Inoshandiswa kune inodzivirira 06Cr19Ni10 uye 06Cr18Ni11Ti zvivakwa zvesimbi isina tsvina ine welding tembiricha inoshanda iri pasi pe300 ° C.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

9.0 ~ 11.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥550

≥35

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Cherechedza:

1. Iyo electrode inofanira kubikwa kweawa imwe panguva inenge 150 ℃ isati yaitwa welding;

2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanira kushandiswa zvakanyanya sezvinobvira kuti ipinde zvakadzama.uye ikozvino haifaniri kunge yakakura zvakanyanya kudzivirira kutsvuka kwetsvimbo yewelding;

3. Kupokana kwekuora uye ferrite yemukati yesimbi yakaiswa inotarirwa nechibvumirano cheviri chekupa uye kudiwa.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.


  • Zvakapfuura:
  • Zvinotevera: