Waya yeAWS A5.7 ERCuSn-C Copper Alloy Welding Wire Brass Welding Wire

Tsananguro pfupi:

Waya yebhuronzi yeAWS A5.7 ERCuSn-C Phosphor inokurudzirwa pakusanganisa mhangura neCu-Sn alloy.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Waya yebhuronzi yeAWS A5.7 ERCuSn-C Phosphor

Nhanganyaya
Zvinokurudzirwa pakusonwa kwemhangura neCu-Sn alloy. Zvakanakisa pakusonwa kwemhangura nesimbi. Zvinokurudzirwa kupisa usati wapisa zvigadzirwa zvakakura, uye kusonwa kwesimbi yesimbi yepulsed argon kunokurudzirwa pakusonwa kwesimbi ine mativi akawanda.

Kugadzirisa:   Chiratidzo cheNhamba:
GB/T9460-2008   SCu5210
AWS A5.7:2007   ERCuSn-C
BS EN14640:2005   Cu 5210
     
Kuumbwa (tsika dzakajairwa):   %
Cu incl.ag   bal.
Zn   0.20
Sn   7.00-9.00
Fe   0.10
P   0.10-0.35
Al   0.01
Pb   0.02
Vamwe vese   0.50
     
Hunhu hwezvinhu:    
Kuwanda kwevanhu Makirogiramu/m3 8.8
Nzvimbo yekunyunguduka ℃ 875-1025
Kufambisa kwekupisa W/mK 66
Kufambisa magetsi Sm/mm2 6-8
Kuwanda kwekuwedzera kwekupisa 10^-6/K(20-300℃) 18.5
     
Maitiro akajairika esimbi inonamirwa:    
Kureba % 20
Simba rekusimba N/mm2 260
Basa rekugadzirisa bha rakachekwa J 32
Kuomarara kweBrinell HB 2.5/62.5 80
     
Mashandisirwo:    
Iron alloy yesimbi ine simbi yakasimba uye yakawedzera kuomarara kwesimbi pakushongedza pamusoro pesimbi. Inonyanya kukodzera kushongedza zvinhu zvemhangura, zvakaita semhangura, tin bronzes, kunyanya zvinoshandiswa pakubatanidza simbi nesimbi dzemhangura. Yakakodzera kushongedza simbi dzakagadzirwa nesimbi uye kusanganisa oven. Kune kushongedza simbi nesimbi, kushongedza simbi nesimbi kunokurudzirwa. Kune simbi hombe dzinoshandiswa pakugadzira zvinhu zvinodziya.
     
Gadzirisa:    
Dhayamita: 0.64 – 0.80 – 1.00 – 1.20 – 1.60 – 2.40
Mapombi: D100, D200, D300, D760, K300, KS300
Tsvimbo: 1.60 - 9.6 mm x 914/1000 mm
Maelectrode anowanikwa.
Zvimwe zvekugadzira kana zvakumbirwa.

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave tichigadzira maerekitironi ekuwelda, tsvimbo dzekuwelda, uye zvinhu zvinoshandiswa pakuwelda kweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira maelectrode esimbi isina ngura, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni & cobalt, mawaya esimbi yekabhoni & low alloy, waya dzesimbi yekabhoni & low alloy, waya dzesimbi yekabhoni, waya dzesimbi yekabhoni, waya dzakavharirwa negesi, waya dzesimbi yekabhoni ...

 

 

 

 


  • Yakapfuura:
  • Zvinotevera: