RBCuZn-B (Nickel Bronze) Brazing Filler Metals Welding Wire

Tsanangudzo Pfupi

RBCuZn-B Nickel Bronze (RBCuZn-B) brazing filler metal yakafanana nebronze yegungwa asi ine manganese nesimbi izvo zvinowedzera kuoma uye kusimba kweweld deposit.


Product Detail

Product Tags

RBCuZn-B Nickel Bronze (RBCuZn-B) brazing filler metal yakafanana nebronze yegungwa asi ine manganese nesimbi izvo zvinowedzera kuoma uye kusimba kweweld deposit.Iyo inewo nickel inovimbisa kugovera kwakafanana kwesimbi mudhipoziti.Murazvo usina kwawakarerekera kana kuti zvishoma oxidizing uye boric acid/boric type flux inofanira kushandiswa.

AWS Kirasi: RBCuZn-B Certification: AWS A5.8/A5.8M:2011
Alloy: RBCuZn-B ASME SFA A5.8

 

Brazing Position: H, V Brazing Range:
1620-1800⁰F

 

Kusimba Simba, kpsi: 60-78
Elongation %, min: 25

 

Melting Point 1620⁰F Solidification 1590⁰F Brinell Hardness 80-110

Typical Wire Chemistry as per AWS A5.8 (single values ​​are maximum)

Cu Zn Sn Fe Mn Ni Pb Al Si Zvimwe
56.0-60.0 Rem 0.80-1.10 0.25-1.20 0.01-0.50 0.20-0.80 0.05 0.01 0.04-0.20 0.50

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 

 

 

 


  • Zvakapfuura:
  • Zvinotevera: