ERCuSn-A (Phos Bronze A) Mhangura uye Copper Alloy Bare Tsvimbo uye Electrodes Tig uye Mig Wire

Tsanangudzo Pfupi

ERCuSn-A Phos Bronze A ibhuronzi yemhangura-zinc ine tin ingangoita 5% uye inosvika 0.35% phosphorus yakawedzerwa se deoxidizer inoshandiswa kusonerera bhuronzi nendarira.


Product Detail

Product Tags

ERCuSn-A Phos Bronze A ibhuronzi yemhangura-zinc ine tin ingangoita 5% uye inosvika 0.35% phosphorus yakawedzerwa se deoxidizer inoshandiswa kusonerera bhuronzi nendarira.Inogonawo kushandiswa kubatanidza mhangura kana kuvapo kwetin musimbi ye weld kusingarambiki.

Typical Applications: pamusoro pesimbi;kujoinha kwe509-519 akatevedzana tin-bronze base masimbi

AWS Kirasi: ERCuSn-A Certification: AWS A5.7/A5.7M:2007
Alloy: ERCuSn-A ASME SFA A5.7

 

Welding Position: Zvazvino:
AC-DCEP

 

Kusimba Simba, kpsi: 35
Brinell Hardness 70-85

Typical Wire Chemistry as per AWS A5.7 ( single values ​​is maximum)

Cu kusanganisira Ag Al Pb P Sn Zvimwe
Remainder 0.01 0.02 0.10-0.35 4.0-6.0 0.50

 

Typical Welding Parameters
Diameter Process Volt Amps GAS
in (mm)
1/16 (1.6) GTAW 70-120 70-150 ACHF kushandisa 100% Argon kana Helium 2% Thoriated, Ceriated kana Lanthanum Tungsten Electrode
3/32 (2.4) GTAW 120-160 140-230 ACHF kushandisa 100% Argon kana Helium 2% Thoriated, Ceriated kana Lanthanum Tungsten Electrode
1/8 (3.2) GTAW 170-230 225-320 ACHF kushandisa 100% Argon kana Helium 2% Thoriated, Ceriated kana Lanthanum Tungsten Electrode
Typical Welding Parameters
Diameter Process Volt Amps GAS
in (mm)
0.035 (1.6) GMAW 20-26 100-200 100% Argon kana 75% Argon, 25% Helium
0.045 (2.4) GMAW 22-28 100-250 100% Argon kana 75% Argon, 25% Helium
1/16 (3.2) GMAW 29-32 250-400 100% Argon kana 75% argon, 25% Helium
3/32 (3.2) GMAW 32-34 350-500 100% Argon kana 75% Argon, 25% Helium

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 

 

 

 