D237 (B-84) Hardfacing Welding Electrode, Surfacing Welding Rod, Arc Welding Stick

Tsanangudzo Pfupi

D237 (B-84) ielectrode yekuputira yakaoma pane alloy steels uye carbon steels.Mabhero ane nzvimbo yakatsetseka, isina makatsemuka uye pores, anoisa zvinhu zvakaomarara zvisingaite abrasion uye zviri pakati nepakati.Easy weld muzvinzvimbo zvese kunze kwakamira pasi.


Product Detail

Product Tags

Hardfacing Welding Stick ElectrodeRODO P

ARA RECUBRIMIENTO MUDZIVIRI

Rudzi Nhamba: D237 (B-84) 

Deposited Metal Analysis (Hunhu chaihwo)

C

Mn

Si

Cr

Mo

V

0.5%

0.3%

0.7%

7%

0.5%

0.5%

 

Hunhu:

B- 84 i electrode yekuomesera yakaomeswa pane alloy simbi uye kabhoni simbi.Mabhero ane nzvimbo yakatsetseka, isina makatsemuka uye pores, anoisa zvinhu zvakaomarara zvisingaite abrasion uye zviri pakati nepakati.Easy weld muzvinzvimbo zvese kunze kwakamira pasi.

Mechanical Properties:Kuoma kubva pa55 kusvika ku60 HRc (yezvikamu)

Welding Positions:Yakati sandarara, Yakachinjika, Pamusoro, Yakatwasuka Kumusoro.

 

Ikozvino uye Polarity:

Yekuchinjanisa kana kunanga ikozvino

Electrode kune iyo yakanaka pole

ø mm

ø in

Amperage

3.20

1/8

100-130

4.00

5/32

120-160

5.00

2/16

180-220

 

Zvishandiso: • Yakanakira kugadzirisa midziyo yekwari, kuunganidza, kuchera

• Laminating mipumburu

• Forging michina

• Michina yekufamba kwePasi

• Kugera mapanga.

 

Urefu: 350mm.

KURERA PABHOKSI: 20 kg / 44 lbs.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo, uye welding consumables kweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 

 

 

 


  • Zvakapfuura:
  • Zvinotevera: