B-85 Hardfacing Welding Electrode, Surfacing Welding Rod, Arc Welding Stick

Tsanangudzo Pfupi

Iko kupfekedzwa kwe electrode iyi kune yakakwira chromium yemukati, iyo inoita kuti dhipoziti yayo isanyanya kupfekwa nekuda kweabrasion yakanyanyisa, kukweshera kwakanyanya uye kuderera, kunyangwe pakupisa kwakanyanya uye mumhepo inoora.Haifanirwe kuratidzwa kuvhunduka kwakanyanya kana kukanganisa.


Product Detail

Product Tags

Hardfacing Welding Stick Electrode

RECUBRIMIENTO MUDZIVIRI

Type Nha.:B – 85

Deposited Metal Analysis (Hunhu chaihwo)

C

4.0%

Si

0.6%

Cr

35%

 

Hunhu:

Iko kupfekedzwa kwe electrode iyi kune yakakwira chromium yemukati, iyo inoita kuti dhipoziti yayo isanyanya kupfekwa nekuda kweabrasion yakanyanyisa, kukweshera kwakanyanya uye kuderera, kunyangwe pakupisa kwakanyanya uye mumhepo inoora.Haifanirwe kuratidzwa kuvhunduka kwakanyanya kana kukanganisa.

 

Mechanical Properties:Kuoma kubva pa57 kusvika ku62 HRc.(Zvivharo zviviri)

 

Ikozvino uye Polarity:

Inodiwa kuchinjanisa ikozvino mune yakananga ikozvino, electrode kune yakanaka pole

ø mm.

1/8”

5/32”

3/16”

Amp.min.

120

170

220

Amp.max.

140

190

250

 

Applications:

• Coat screw conveyors

• Mabhakiti ekuchera

• Mazino anokuvadza

• Dredge pombi

• Michina yekuchera

• Mapombi ejecha

 

 

Urefu: 350mm.

KURERA PABHOKSI: 20 kg / 44 lbs.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo, uye welding consumables kweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 

 

 

 


  • Zvakapfuura:
  • Zvinotevera: