AWS A5.4 E309L-16 Stainless Steel Welding Rods Best Welding Electrode

Tsanangudzo Pfupi

A062 (AWS E309L-16) ndeye Ultra-low kabhoni Cr23Ni13 Stainless simbi electrode ine titanium-calcium coating.


Product Detail

Product Tags

Stainless Simbi Welding Electrode

A062                                         

GB/T E309L-16

AWS E309L-16

Tsanangudzo: A062 is an ultra-low carbon Cr23Ni13 Stainless steel electrode ine titanium-calcium coating.Inogona kushandiswa kune ese AC uye DC.Iyo ine yakaderera kabhoni yemukati, saka inokwanisa kuramba intergranular corrosion inokonzerwa nekunaya kwecarbide isina zvigadzikiso senge niobium uye titanium.

Chishandiso: Inoshandiswa kune imwecheteyo mhando yesimbi isina simbi chimiro, inoumbwa simbi, uye yakakosha-yakaita simbi zvikamu mukugadzirwa kwesynthetic fiber, petrochemical, uye zvimwe midziyo.Inogona zvakare kushandiswa kukwirisa kwezvikamu zvekuchinja pamadziro emukati menyukireya reactor pressure midziyo uye welding ye tower internals.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥520

≥25

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~ 70

80 ~ 110

130 ~ 160

160 ~ 200

 

Cherechedza:

1. Iyo electrode inofanira kubikwa kweawa imwe panguva inenge 150 ℃ isati yaitwa welding;

2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanira kushandiswa zvakanyanya sezvinobvira kuti ipinde zvakadzama.uye ikozvino haifaniri kunge yakakura zvakanyanya kudzivirira kutsvuka kwetsvimbo yewelding

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

OEM / ODM:

Isu tinotsigira OEM / ODM uye tinogona kuita chibvumirano chekutakura kune dhizaini yako, ndapota taura nesu kuti tikurukure zvakadzama.


  • Zvakapfuura:
  • Zvinotevera: