AWS A5.4 E309-16 Stainless Steel Welding Electrode Welding Consumables Welding Materials, Welding Stick

Tsanangudzo Pfupi

A302 (AWS E309-16) iCr23Ni13 Stainless steel electrode ine titanium-calcium coating.


Product Detail

Product Tags

Stainless Simbi Welding Electrode

A302                                      

GB/T E309-16

AWS A5.4 E309-16

Tsanangudzo: A302 iCr23Ni13 Stainless steel electrode ine titanium-calcium coating.Inogona kushandiswa kune ese AC uye DC ine yakanakisa mashandiro ekushanda.Iyo simbi yakaiswa ine yakakura kuramba kutsemuka uye oxidation kuramba.

Chishandiso: Inoshandiswa kupinza mhando imwechete yesimbi isina tsvina, simbi isina tsvina, simbi yakasarudzika (Cr19Ni9 yakafanana nekabhoni simbi yakaderera), yakakwirira chromium simbi, yakakwirira manganese simbi, nezvimwe.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

2.0 ~ 4.0

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥550

≥25

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Cherechedza:

1. Iyo electrode inofanira kubikwa kweawa 1 pa 150 ℃ isati yaitwa welding;

2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanira kushandiswa zvakanyanya sezvinobvira kuti ipinde zvakadzama.uye ikozvino haifaniri kunge yakakura zvakanyanya kudzivirira kutsvuka kwetsvimbo yewelding.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.


  • Zvakapfuura:
  • Zvinotevera: