AWS A5.1 E7028 Welding Tsvimbo Iron Powder uye Yakaderera Hydrogen Stick Electrodes yeArc Welding

Tsanangudzo Pfupi

J501Fe13 (AWS E7028) inonzi carbon steel electrode ine iron powder uye yakaderera hydrogen potassium coating.


Product Detail

Product Tags

Carbon Steel Welding Electrode

J506Fe13

GB/T E5028

AWS A5.1 E7028

Tsanangudzo: J501Fe13 inonzi carbon steel electrode ine iron powder uye yakaderera hydrogen potassium coating.AC uye DC zvine mbiri-chinangwa, inokodzera flat welding uye flat fillet welding.Iyo deposition kunyatsoshanda kwakatenderedza 130%.

Chikumbiro: Inoshandiswa kune flat welding uye flat angle welding yekabhoni simbi uye yakaderera alloy simbi, senge Q345, nezvimwe.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

S

P

≤0.12

≤1.60

≤0.75

≤0.035

≤0.035

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Goho simba

Mpa

Elongation

%

Impact value (J)

(-46℃)

Guaranteed

≥490

≥400

≥22

≥27

 

Diffusion hydrogen zvemukati mesimbi yakaiswa: ≤8.0mL/100g (glycerin nzira)

 

X-ray kuongorora: II giredhi

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

4.0

5.0

Welding ikozvino

(A)

180 ~ 220

210 ~ 260

 

Cherechedza:

1.Iyo electrode inofanira kubikwa kweawa 1 pa 350 ℃ isati yaitwa welding;

2. Zvinokosha kuchenesa ngura, chikero chemafuta, mvura, uye tsvina pazvikamu zvewelding tisati tasveta.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 


  • Zvakapfuura:
  • Zvinotevera: