E6010 carbon steel welding electrode

Tsananguro pfupi:

E6010 ielectrode yerudzi rwe rutile-cellulosic sodium.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

AWS E6010 Electrode Yekushongedza Simbi Yakapfava

ZVINOSHANDISWA:

Yakakodzera kusanganisa simbi ine kabhoni shoma semapaipi, kuvaka ngarava uye zambuko nezvimwewo.

KUGADZIRWA KWEMAHARA:

AWS A5.1 / ASME SFA5.1 E6010

JIS Z3211 D4310

HUNHU:

E6010 ielectrode yemhando yesodium inonzi rutile-cellulosic. Inogona kusungirirwa panzvimbo yese (kunyanya panzvimbo yakamira-pasi) neDC+ chete. Ine mashandiro akanaka ekushongedza searc yakagadzikana, kupfapfaidza kudiki, kubvisa tsvina nyore nyore uye kugona kudzoreredza simba nezvimwewo. Kudzora dziva rakanyungudutswa kuri nani, simba rakasimba rearc uye kupinda kwakadzika panzvimbo yakamira-pasi.

KUUMBIKA KWEMAKEMIKIRI EMAWELDS OSE SIMBIRI: (HW. %)

Zvinhu C Mn Si S P Ni Cr Mo V
Zvinodiwa ≤0.20 0.3-0.6 ≤0.30 ≤0.035 ≤0.040 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Mhedzisiro Yakajairika 0.09 0.48 0.23 0.020 0.025 0.030 0.035 0.005 0.004

ZVINHU ZVEMAKANIKISI ZVINOWEDZERWA SIMBIRI:

Zvinhu Rm/MPa Rel/Rp0.2 /MPa A/% KV2 (-30℃) /J
Zvinodiwa ≥430 ≥330 ≥20 ≥27
Mhedzisiro Yakajairika 475 400 26 80

TARISIRO:

1. Kazhinji, haufanirwe kuomesa electrode zvakare usati waibatanidza. Kana yakanganiswa neunyoro, inofanira kuomesa zvakare pa70℃-90℃ kweawa imwe chete.

2. Ngura, mafuta, mvura nezvimwe tsvina zviri munzvimbo yekunamira zvinofanirwa kubviswa zvisati zvanamira.

MAITIRO EKUSHANDA AIWANZO: (DC+)

Dhayamita (mm) 2.5 3.2 4.0 5.0
Kureba (mm) 300 350 400 400
Ikozvino (A) 50-80 60-100 100-140 140-180

KUPAKISHA:

5kg/bhokisi, mabhokisi mana/bhokisi, 20kgs/bhokisi, 50mabhokisi/pallet. 21MT -26MT pa 1X20″ FCL.

 

OEM/ODM:

Tinotsigira OEM/ODM uye tinogona kugadzira machira zvichienderana nedhizaini yenyu, ndapota taurai nesu kuti tikurukure zvakadzama.

 

Hunhu paMashandisirwo:

Arc yakasimba kwazvo.

Kubviswa kwakanaka kwetsvina.

Kupinda mukati hakuna kudzika.

Kudzivirira kupisa nekuora zvakanaka.

Kudzivirira kutsemuka kwakanaka.


  • Yakapfuura:
  • Zvinotevera: