E316L-16 Electrode yesimbi isina ngura

Tsananguro pfupi:

E316L-16 Kukwesha kabhoni yakaderera zvakanyanya 18%Cr-12%Ni-2%Mo (316L simbi isingatsvi)


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

AWS A5.4 E316L-16 Tsvimbo dzeWelding dzeSimbi Isina Stainless

AWS: SFA 5.4 E316L-16

IS: 5206 E19.12.2.LR16

EN ISO CODE: 3581-AE 19 12 3 LR 3 2

Hunhu paKushandiswa:

E316L-16 ielectrode yerudzi rwe lime-titania ine mashandisirwo akanaka uye inochinjika.

Sezvo simbi iyi ine chimiro che austenite chine huwandu hwakakwana hwe ferrite, kugona kudzima matombo kwakanaka. Inokwanisa kudzima ngura ye intercrystalline mumamiriro ezvinhu akasungirirwa sezvo kabhoni iri shoma uye kugona kudzima ngura ye intergranular kuri nani pane E316L-16 uye ine Mo. Kugona kudzima kupisa kwakanakawo.

E316L-16 ine hunyoro hwakanyanya uye inogona kudzikamisa maburi zvakanaka.

KUUMBIKA KWEMAKEMIKIRI YESIMBIRI YEWELD (%)

Chinhu

C

Mn

Si

Cr

Ni

Mo

S

P

Cu

Chikamu

≤0.04

0.50-2.50

≤0.90

17-22

11-14

2.0-3.0

≤0.030

≤0.04

≤0.75

ZVINHU ZVEMAKANIKISI ZVINOWEDZERWA SIMBIRI

UTS

Kureba

(MPa)

(L= 5d)%

545

40

DATA RAVA PARIZVINO UYE ROKUPAKISA: AC / DC(+)

Saizi (mm)

5×350

4×350

3.15×350

2.5×350

Range yeParizvino (Amps)

150-180

110-140

80-100

60-80

Kurema / Katoni (kgs)

2.5

2.5

2.5

2.5

Kungwarira:

1. Shandisa arc pfupi ne stringer bead kuderedza kupisa.

2. Iva nechokwadi chekuti maerekitirodhi akaoma. Omesai maerekitirodhi zvakare pa 250-300°C kweawa imwe chete.

Zvinyorwa paMashandisirwo:

Upamhi hwekuruka hunofanira kunge huri mukati mehupamhi hwemaelektrode kaviri nehafu.

Bvisa tsvina yakaita semafuta neguruva kubva pamugero.

Omesa maerekitirodhi pa350 (662) kwemaminitsi makumi matanhatu usati washandisa.