AWS E316-15 Stainless Steel Welding Electrode Arc Welding tsvimbo dzeManual Welding

Tsanangudzo Pfupi

A207 (AWS E316-15) i-low-carbon Cr18Ni12Mo2 Stainless steel electrode ine low-hydrogen sodium coating.


Product Detail

Product Tags

Stainless Simbi WeldingElectrode

A207                                      

GB/T E316-15

AWS E316-15

Tsanangudzo: A207 i-low-carbon Cr18Ni12Mo2 Stainless steel electrode ine yakaderera-hydrogen sodium coating.Shandisa DCEP (yakananga ikozvino electrode yakanaka) uye inogona kusungirirwa munzvimbo dzese.Sezvo simbi yakaiswa iine molybdenum, ine huturu hwekuora, kupikisa kupisa uye kuramba kutsemuka, kunyanya yakanakira kurwisa chloride ion pitting corrosion.

Chikumbiro: Inoshandiswa kukwenenzvera low-carbon 06Cr17Ni12Mo2 Stainless simbi zvivakwa, pamwe nepamusoro-chromium simbi (senge Cr13, Cr17, zvichingodaro) izvo zvisingadi kurapwa kwekupisa mushure mekupinza, uye welding yesimbi dzakasiyana.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥520

≥30

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

Cherechedza:

  1. Iyo electrode inofanira kubikwa kweawa imwe painotenderera 250 ℃ isati yaitwa welding.Usabika kakawanda.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo,uyewelding zvinodyiwakweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.