AWS E317-16 Stainless Steel Welding tsvimbo Arc Welding Stcik Welding Electrodes

Tsanangudzo Pfupi

A242 (AWS E317-16) is a low-carbon Cr19Ni13Mo3 Stainless steel electrode ine titanium-calcium coating.


Product Detail

Product Tags

Stainless Simbi WeldingElectrode

A242                                      

GB/T E317-16

AWS A5.4 E317-16

Tsanangudzo: A242 i-low-carbon Cr19Ni13Mo3 Stainless steel electrode ine titanium-calcium coating.Inogona kushandiswa kune ese AC uye DC ine yakanakisa mashandiro ekushanda.Simbi yakaiswa ine yakakwira molybdenum yemukati kupfuura A202, uye ine zvirinani kusagadzika kwecorrosion kune asiri-oxidizing acid, senge sulfuric acid, sulfurous acid, phosphoric acid uye organic acids.Iyo ine zvakare mhedzisiro yakanaka pakurwisa corrosion.

Chishandiso: Inoshandiswa pakuputira mhando imwechete yemidziyo yesimbi isina tsvina pamwe chete nesimbi inoumbwa nesimbi isina kufanana.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

2.0 ~ 4.0

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥550

≥25

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Cherechedza:

1. Iyo electrode inofanira kubikwa kweawa 1 pa 150 ℃ isati yaitwa welding;

2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanira kushandiswa zvakanyanya sezvinobvira kuti ipinde zvakadzama.uye ikozvino haifaniri kunge yakakura zvakanyanya kudzivirira kutsvuka kwetsvimbo yewelding.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo,uyewelding zvinodyiwakweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira simbi isina tsvinawelding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminium welding wires, submerged arc welding. .waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 


  • Zvakapfuura:
  • Zvinotevera: