Welding Electrode AWS A5.4 E310Mo-16 Stainless Steel Welding Tsvimbo Electrodes

Tsanangudzo Pfupi

A412 (AWS E310Mo-16) iCr26Ni21Mo2 pure austenitic stainless steel electrode ine titanium calcium coating.


Product Detail

Product Tags

Stainless Simbi WeldingElectrode

A412                                 

GB/T E310Mo-16

AWS A5.4 E310Mo-16

Tsanangudzo: A412 ndeye Cr26Ni21Mo2 pure austenitic Stainless steel electrode ine titanium calcium coating.Inogona kushandiswa kune ese AC uye DC ine yakanakisa mashandiro ekushanda.Nekuti molybdenum inowedzerwa kusimbi yakaiswa, kupikisa kwayo kwegomba, simba rekupisa uye kuramba kwekuputika zvese zvinovandudzwa zvichienzaniswa neA402 neA407.

Chikumbiro: Inoshandiswa kugadzira kupisa-inodzivirira simbi isina tsvina inoshanda pasi pemamiriro ekushisa kwepamusoro, uye inogonawo kushandiswa kugadzira simbi isina tsvina, simbi dzakasiyana-siyana, nezvimwewo. Iine kutsemuka kuri nani kana welding kabhoni simbi uye yakaderera alloy simbi ine yakakwirira kuoma. .

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

1.0 ~ 2.5

≤0.75

25.0 ~ 28.0

20.0 ~ 22.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.030

 

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥550

≥25

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Cherechedza:

  1. Iyo electrode inofanira kubikwa kweawa imwe panguva yakatenderedza 150 ℃ isati yaitwa welding;
  2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanirwa kushandiswa zvakanyanya sezvinobvira kuwana yakadzika kupinda.uye ikozvino haifaniri kunge yakakura zvakanyanya kudzivirira kutsvuka kwetsvimbo yewelding.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo,uyewelding zvinodyiwakweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 

 

 


  • Zvakapfuura:
  • Zvinotevera: