Stainless Steel Arc Welding Tsvimbo AWS A5.4 E310H-16 Yakanyanya Hunhu Welding Electrode Supplier

Tsanangudzo Pfupi

A432 (AWS A5.4 E310H-16) ndeye 3Cr26Ni21 inodzivirira kupisa inodzivirira Stainless simbi electrode ine titanium-calcium coating.


Product Detail

Product Tags

Stainless Simbi WeldingElectrode

A432                                 

GB/T E310H-16

AWS A5.4 E310H-16

Tsanangudzo: A432 ndeye 3Cr26Ni21 inodzivirira kupisa inodzivirira Stainless simbi electrode ine titanium-calcium coating.Inogona kushandiswa kune ese AC uye DC ine yakanakisa mashandiro ekushanda.Simbi yakaiswa ine yakakwira simba rekudonha, kuita kwakanaka kwemajoini, uye kuderera kwekushisa kwekunzwa kwekuputika.

Chikumbiro: Inonyanya kushandiswa kugadzira HK40 inodzivirira kupisa simbi.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Cr

Ni

Mo

Mn

Si

Cu

S

P

0.35 ~ 0.45

25.0 ~ 28.0

20.0 ~ 22.5

≤0.75

1.0 ~ 2.5

≤0.75

≤0.75

≤0.030

≤0.030

 

Mechanical zvimiro zve weld simbi:

Test chinhu

 

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥620

≥10

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

3.2

4.0

5.0

Welding Current

(A)

80 ~ 110

110 ~ 160

160 ~ 200

 

Cherechedza:

  1. Iyo electrode inofanira kubikwa kweawa imwe panguva yakakomberedza 150 ℃ isati yaitwa welding;
  2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanirwa kushandiswa zvakanyanya sezvinobvira kuwana yakadzika kupinda.uye ikozvino haifaniri kunge yakakura zvakanyanya kudzivirira kutsvuka kwetsvimbo yewelding.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo,uyewelding zvinodyiwakweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira simbi isina tsvinawelding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminium welding wires, submerged arc welding. .waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 


  • Zvakapfuura:
  • Zvinotevera: