ER5356 Aluminium Welding Wire Welding Tsvimbo uye Electrodes

Tsanangudzo Pfupi

ER5356 ndeye general-chinangwa mhando aruminiyamu alloy iyo inowanzo sarudzirwa kusimba kwayo kwekugera.


Product Detail

Product Tags

ER5356 ndeye general-chinangwa mhando aruminiyamu alloy iyo inowanzo sarudzirwa kusimba kwayo kwekugera.Pamusoro pezvo, inopawo yakanakisa corrosion resistance kana yaiswa mumvura yemunyu.ER5356 inofanira kutariswa kune welding 5000 akatevedzana aruminiyamu base simbi.

Typical Applications: welding filler waya

AWS Kirasi: ER5356 Certification: AWS A5.10/ A5.10M:1999
Alloy: ER5356 AWS/ASME SFA A5.10
Welding Position:
F, V, H
Zvazvino:
DCEP-GMAW
AC-GTAW
Yakajairika Properties (seyakaiswa welded)
Conductivity: 29% IACS (-0)/27% IACS (-H18)
Kusimba Simba, kpsi: 38
Ruvara: Chena
Melting Point 1175⁰F Solidification 1060⁰F Density 0.096 lbs/cu In.
Typical Wire Chemistry as per AWS A5.10 ( single values ​​is maximum)
Si Fe Cu Mn Mg Cr Zn Ti Zvimwe AL
0.25 0.40 0.10 0.50-1.0 4.7-5.5 0.05-0.20 0.25 0.05-0.20 0.15 Remainder
Typical Welding Parameters
Diameter Process Volt Amps GAS
in (mm)
.030 (.8) GMAW 15-24 60-175 Argon (cfh)
.035 (.9) GMAW 15-27 70-185 Argon (cfh)
3/64” (1.2) GMAW 20-29 125-260 Argon (cfh)
1/16” (1.6) GMAW 24-30 170-300 Argon (cfh)
3/32” (2.4) GMAW 26-31 275-400 Argon (cfh)
Diameter Process Volt Amps GAS
in (mm)
1/16” (1.6) GTAW 15 60-80 Argon (cfh)
3/32” (2.4) GTAW 15 125-160 Argon (cfh)
1/8” (3.2) GTAW 15 190-220 Argon (cfh)
5/32” (4.0) GTAW 15 200-300 Argon (cfh)
3/16” (4.8) GTAW 15-20 330-380 Argon (cfh)

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 

 