AWS ER5183 Aluminium Welding Wire Aluminium MIG welding tsvimbo uye Tig Wire

Tsanangudzo Pfupi

ER5183 inokodzera MIG welding iyo aruminiyamu magnesium alloy iyo yakakwirira tensile simba inodiwa uye kana base simbi iri 5083 kana 5654 iyo tensile simba ingave yakakwira zvakanyanya.Inoshandiswa zvakanyanya kugadzira aluminium magnesium alloy zvimiro zvezvikepe, offshore mapuratifomu, locomotives & ngoro, mota mota, midziyo, cryogenic ngarava uye zvichingodaro.


Product Detail

Product Tags

ER5183 inokodzera MIG welding iyo aruminiyamu magnesium alloy iyo yakakwirira tensile simba inodiwa uye kana base simbi iri 5083 kana 5654 iyo tensile simba ingave yakakwira zvakanyanya.Inoshandiswa zvakanyanya kugadzira aluminium magnesium alloy zvimiro zvezvikepe, offshore mapuratifomu, locomotives & ngoro, mota mota, midziyo, cryogenic ngarava uye zvichingodaro.Simbi yaro ye weld ine kumira kwakanaka kune brine corrosion.

Welding Position: F, HF, V

Rudzi Rwazvino: DCEP

CHIZIVISO:

Kuchengeta pasuru yewaya iri muchimiro chakanaka usati welding.

Idzo mbiri nzvimbo dzinofanirwa kusungirirwa weldment uye waya dzinofanirwa kucheneswa kure nekusvibiswa kwekusvibiswa kwemafuta, oxide coating, mwando uye zvichingodaro.

Kuti uwane chitarisiko chakanaka che weld inodiwa preheat base simbi kusvika 100 ℃-200 ℃ isati yave welding kana ukobvu hwayo huri 10mm kana kupfuura.

Zviri nani kuisa subplate pasi peiyo weld zone kuti utsigire simbi yakanyunguduka kuitira kuti uve nechokwadi chekupinda kwakazara kweweldment.

Zvinoenderana nenzvimbo yewelding uye ukobvu hwesimbi yesimbi yakasiyana nhovo gasi inofanirwa kusarudzwa, senge 100% Ar, 75% Ar + 25% Iye, 50% Ar + 50% Iye, nezvimwe.

Mamiriro emagetsi ataurwa pamusoro apa kuti aonekwe chete uye zviri nani kuita welding process qualification maererano nepurojekiti usati waisa mu welding yepamutemo.

ER5183 CHEMICAL COMPOSITION OF DEPOSITED METAL (%):

SI FE CU MN MG CR ZN TI AI BE
Standard ≤0.40 ≤0.40 ≤0.10 0.50-10 4.3-52 0.05-0.5 ≤0.25 ≤0.15 Balance ≤0.0003
Typical 0.08 0.12 0.006 0.65 4.75 0.130 0.005 0.080 Balance 0.0001

MACHANICAL PROPERTIES OF DEPOSITED METAL (AW):

TENSILE SIMBA RM (MPA) YIELD SIMBA REL (MPA) ELONGATION A4 (%)
Typical 280 150 18

Saizi & Zvinokurudzirwa Zvazvino zveMIG (DC+):

WELDING WAYA DIAMETER (MM) 1.2 1.6 2.0
Welding Current (A) 180-300 200-400 240-450
Welding Voltage (V) 18-28 20-20 22-34

MAUKURU & AKAKURUKURWA ZVINO KUTI TIG (DC¯):

WELDING WAYA DIAMETER (MM) 1.6-2.5 2.5-4.0 4.0-5.0
Welding Current (A) 150-250 200-320 220-400

 

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 

 


  • Zvakapfuura:
  • Zvinotevera: