AWS E8016-G Welding Electrodes Low Alloy Steel Welding Rods Stick Arc Welding Materials

Tsananguro pfupi:

J556 (AWS E8016-G) ielectrode yesimbi ine alloy yakaderera ine hydrogen potassium yakaderera. AC neDC zvese zvinogona kushandiswa, uye zvinogona kusungirirwa munzvimbo dzese.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Electrode Yesimbi Yekushongedza Yesimbi Yakaderera

J556

GB/T E5516-G

AWS E8016-G

Tsananguro: J556 ielectrode yesimbi ine alloy yakaderera ine hydrogen potassium yakaderera. AC neDC zvese zvinogona kushandiswa, uye zvinogona kusungirirwa munzvimbo dzese. Kugadzikana kwekushanda kweAC welding kwakaderera zvishoma pane kwe direct welding.

Mashandisirwo: Inoshandiswa pakusanganisa simbi yekabhoni iri pakati nepakati uye simbi ine alloy yakaderera senge Q390.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Si

S

P

≤0.12

≥1.00

0.30 ~ 0.70

≤0.035

≤0.035

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Kukosha kwemhedzisiro (J)

-30℃

Yakavimbiswa

≥540

≥440

≥17

≥27

Yakaedzwa

550 ~ 620

≥450

22 ~ 32

—

 

Kupararira kwehydrogen musimbi yakachengetwa: ≤6.0mL/100g (nzira yeglycerin)

 

Kuongororwa kweX-ray: Giredhi I

 

Inokurudzirwa yemagetsi:

Dhayamita yetsvimbo

()mm)

2.5

3.2

4.0

5.0

Welding current

()A)

60 ~ 90

80 ~ 110

130 ~ 170

160 ~ 200

 

Cherechedza:

1. Electrode inofanira kubikwa kweawa imwe pa350℃ isati yashandiswa pakunamira;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira;

3. Shandisa arc operation pfupi pakusanganisa. Nzira yakamanikana yekusanganisa ndiyo yakakodzera;

4. Batanidza electrode ku positive pole kana uchishanda paDC.

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave tichigadzira maerekitironi ekuwelda, tsvimbo dzekuwelda, uye zvinhu zvinoshandiswa pakuwelda kweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira maelectrode esimbi isina ngura, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni & cobalt, mawaya esimbi yekabhoni & low alloy, waya dzesimbi yekabhoni & low alloy, waya dzesimbi yekabhoni, waya dzesimbi yekabhoni, waya dzakavharirwa negesi, waya dzesimbi yekabhoni ...

 