Tsanangudzo Pfupi

A042(AWS E309MoL-16) is an ultra-low carbon Cr23Ni13Mo2 Stainless steel electrode ine titanium calcium coating.


Product Detail

Product Tags

Stainless Simbi WeldingElectrode

A042                                         

GB/T E309MoL-16

AWS E309MoL-16

Tsanangudzo: A042 is an ultra-low carbon Cr23Ni13Mo2 Stainless steel electrode ine titanium calcium coating.Inogona kushandiswa kune ese AC uye DC.Nekuda kwekuwedzera kwehuwandu hwakakodzera hwemolybdenum, kutsemuka kwekusagadzikana uye kushora kwesimbi yesimbi yakaiswa kunovandudzwa.

Chishandiso: Kune imwecheteyo mhando ye Ultra-yakaderera kabhoni Stainless simbi zvinhu (senge urea synthesis tower lining) uye dissimilar simbi welding, nezvimwe.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥520

≥25

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Cherechedza:

1. Iyo electrode inofanira kubikwa kweawa imwe panguva inenge 150 ℃ isati yaitwa welding;

2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanira kushandiswa zvakanyanya sezvinobvira kuti ipinde zvakadzama.uye ikozvino haifaniri kunge yakakura zvakanyanya kudzivirira kutsvuka kwetsvimbo yewelding;

3.Kurwisana kwekuora kwesimbi yakaiswa kunotsanangurwa nechibvumirano chechipiri chekugovera uye kudiwa.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo,uyewelding zvinodyiwakweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira simbi isina tsvinawelding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminium welding wires, submerged arc welding. .waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.


  • Zvakapfuura:
  • Zvinotevera: