AWS ENiCrFe-4 Nickel Alloy Welding Electrodes yeShielded Metal Arc Welding, Welding tsvimbo

Tsanangudzo Pfupi

Ni307-4 (AWS ENiCrFe-4) is nickel-based electrode ine yakaderera-hydrogen sodium coating.Shandisa DCEP (yakananga ikozvino electrode yakanaka).


Product Detail

Product Tags

Nickel uyeNickel Alloy Welding Electrode

Ni307-4                                                     

GB/T ENi6093

AWS A5.11 ENCrFe-4

 

Tsanangudzo: Ni307-4 is nickel-based electrode ine yakaderera-hydrogen sodium coating.Shandisa DCEP (yakananga ikozvino electrodepositive).Iyo ine yakanakisa welding performance ine yakagadzikana arc combustion, shoma spatter, nyore kubvisa slag,

uye weld yakanaka.

 

Chikumbiro:Iyo inoshandiswa kugadzira nickel-chromium-iron alloys, yakadai seNi600, Ni800/800H uye yakafanana kana nickel-based superalloys ine tembiricha yekushanda ye900 ° C. Inogona zvakare kushandiswa kune yakaderera-tembiricha masimbi ane Ni3% ~ 9%, yakadai seASTM A333, A334, A353, A522, The welding of A553 inogonawo kushandiswa kune dissimilar metal welding pakati peMo400, Ni825, simbi isina tsvina uye yakaderera alloy simbi.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Fe

Si

Ni

Cr

Mo

Nb + Ta

S

P

≤0.20

1.0 ~ 5.0

≤12.0

≤1.0

≥60.0

13.0 ~ 17.0

1.0 ~ 3.5

1.0 ~ 3.5

≤0.015

≤0.020

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Goho simba

Mpa

Elongation

%

Guaranteed

≥650

≥360

≥18

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

Welding ikozvino

(A)

60 ~ 90

80 ~ 110

110 ~ 150

 

Cherechedza:

1. Elekitirodhi inofanira kubikwa kweawa imwe panguva inenge 300 ℃ isati yaitwa welding;

2. Zvakakosha kuchenesa dzine ngura, oiri, mvura, uye tsvina pazvikamu zvinonamatwa tisati tapisa.Edza kushandisa arc pfupi kuti weld.

 

 