ENiCrFe-3 Electrodes eNickel

Tsananguro pfupi:

Electrode iri kuisa simbi ye65Ni-20Cr-2Nb-1.5Mo.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

EN ISO CODE: 14172:ENi6082

Electrode iri kuisa simbi ye65Ni-20Cr-2Nb-1.5Mo yeweld. Simbi yeweld yemhando yepamusoro ine hunhu hweRadiographic. Yakakodzera kwazvo ku welding alloys dzakafanana nedzayo, yekuisa pamusoro pesimbi ine Nickel-Chromium-Iron alloy kana zvinhu zvakawanda zveManganese zvisina kuipa, yekubatanidza simbi yeNickel Chromium-Iron nesimbi dzakasiyana. Yakakodzera kufukidza ma forge plates. Inokurudzirwa zvikuru pakuwelding 9% Ni Steels yebasa re cryogenic. Inoshandiswawo pakuwelding Nickel-Chromium alloys dzinoshandiswa pakushandiswa kwekupisa kwakanyanya senge zvinhu zvinodziya muchoto nemachubhu ekugadzirisa.

Kuumbwa kwemakemikari kwakajairika kwesimbi yese yesimbi yesimbi

Chinhu C Mn Si Cr Ni Fe Nb Cu Ti S P
Chikamu ≤0.10 5.0-9.5 ≤1.0 13.0-17.0 ≥59.0 ≤10.0 1.0-2.5 ≤0.50 ≤1.0 ≤0.015 ≤0.030

ZVINHU ZVEMAKANIKISI ZVAKAJAIRWA ZVESIMBIRI YEWELD

UTS YS Kureba Simba reCVN (J) Kuwedzera Kwemativi Simba reKukwira pa
(MPa) (MPa) (L= 5d)% pa 196°C pa 196°C (mm) 600°C kwemaawa chiuru.
620 500 30 75 0.85 160 MPa

DATA REKUKURUMIDZA UYE ROKUPAKISA: DC (+)

Saizi (mm)

Kureba kweDia x

5×350

4×350

3.15×350

2.5×350

Range yeParizvino (Amps)

150-180

120-150

80-110

60-70

Kurema/Bhokisi (kgs)

2.5

2.5

2.5

2.5

Kungwarira

1. Iva nechokwadi chekuti maerekitirodhi akaoma. Omesai maerekitirodhi zvakare pa300-325°C kweawa imwe chete.

2. Chengetedza tambo pfupi, tambo dzakaita setambo uye deredza kupisa.

3. Rega weld itonhore kusvika pasi pe50 C usati waisa, wedzera chikamu chinotevera.


  • Yakapfuura:
  • Zvinotevera: