Tsananguro pfupi:

Electrode yekuwedera yemhando yetitanium yesimbi isina ngura ine kabhoni shoma.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Kupatsanura:

AWS A5.4 / ASME SFA5.4 E308-16

JIS Z3221 D308-16

Tsananguro:

Electrode Yekushongedza Simbi Isina StainlessE308-16 rudzi rwetitanium yemutsaraelectrode yekunamirayesimbi isina ngura ine kabhoni shoma. Simbi iyi ine hunhu hwakanaka hwemakanika uye inodzivirira ngura yepakati pegranular nekuda kwekuti kabhoni iri mairi iri ≤. 0.04% b. Inogona kushandiswa pakushongedza nzvimbo dzese nekushanda kwakanaka: arc yakagadzikana, masmatter madiki, chitarisiko chakanaka chekushongedza. Uye zvakareelectrode yekunamiraInodzivirira kupisa zvakanaka, haisi nyore kutsvuka uye gasi harigadzike.

Kushandiswa:

Kukwesha simbi ye18%Cr-8%Ni.

Yakakodzera zvivakwa zvekunamira zvakagadzirwa nesimbi isina ngura ine kabhoni shoma 022Cr-19Ni10, senge fiber yekugadzira, fetiraiza,

michina yepetrochemical, nezvimwewo.

Kuumbwa kweMakemikari eSimbi Yakachengetwa (E308L-16) (%)

Chinhu C Mn Si Cr Ni S P Cu Mo
kukosha kwakajairika ≤0.08 0.5-2.5 ≤0.90 18.0-21.0 9.0-11.0 ≤0.030 ≤0.040 ≤0.75 ≤0.75
Muenzaniso wekukosha 0.043 1.10 0.78 19.52 9.76 0.012 0.031 0.02 0.032

Hunhu hweMechanical hweSimbi Yakachengetwa (%)

Kushanda kwekudzivirira ngura uye kuumbwa kweferrite zvinofanirwa kusarudzwa pakati pemutengi nemutengesi.

Chinhu Simba reKusimba (MPa) Kureba (%)
kukosha kwakajairika ≥550 ≥25
Muenzaniso wekukosha 601 41

Dhayamita (mm)

2.0

2.5

3.2

4.0

5.0

Kuwedera Kwemagetsi (A)

25-50

50-80

80-110

110-160

160-200

 

Zvinyorwa paMashandisirwo:

1. Chengeta arc iri pfupi sezvinobvira.

2. Bvisa tsvina yakaita semafuta neguruva kubva pamugero.

3. Omesa maerekitirodhi pa350 (662) kwemaminitsi makumi matanhatu usati washandisa.