TYUE E7018 CARBON STEEL ELECTRODE

Tsananguro pfupi:

Electrode yesimbi yesimbi ine hydrogen yakaderera potassium yakaputirwa necarbon steel.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Kupatsanura:

AWS A5.1 E7018

ISO 2560-B-E4918A

GB/T 5117 E5018

Tsvimbo dzeWelding AWS E7018 ielectrode yesimbi ine hydrogen iron potassium powder yakaderera. Guruva resimbi riri mu coating rinowedzera mwero we deposit rate. Rine mukana wakanaka wekushandisa zvinoita kuti rive ne arc yakagadzikana, slatter shoma, kubvisa slag kuri nyore uye sveld munzvimbo dzese. Simbi yakachengetwa ine hunhu hwakanaka hwemakanika hune simba rakanaka kwazvo pakupisa kwakaderera.

Kuumbwa kwemakemikari (%)
Kuumbwa kweMakemikari

C

Mn

Si

S

P

Kukosha kweVimbiso

≤0.12

≤1.60

≤0.75

≤0.035

≤0.040

Mhedzisiro Yese

0.089

1.2

0.38

0.028

0.04

Hunhu hwesimbi yakachengetwa muchimiro chemakanika
Chinhu Chekuyedza

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) -30°C

Kukosha kweVimbiso

≥490

≥400

≥20

≥27

Mhedzisiro Yese

515

430

32

156

Referensi yemazuva ano (DC)

Dhayamita

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

60 ~ 100

80 ~ 140

110 ~ 210

160 ~ 230

Nzvimbo Yekushongedza:

PA, PB, PC, PD, PE, PF

Zvinyorwa:
1. Electrode inofanira kupisa patembiricha ye350°C kweawa imwe chete. Pisa tsvimbo pese painoshandiswa.
2. Tsvina yakaita sengura, mavara emafuta uye hunyoro zvinofanirwa kubviswa pabasa.
3. Mutsetse mupfupi unodiwa pakupinza simbi. Nzira yakamanikana yekupinza simbi ndiyo inofarirwa.

 

Kuchenjerera:

  1. Telectrode inofanira kuomeswa patsva ne350℃-380℃kweawa imwe chete usati wabatanidza.
  2. Tmafuta, mvura nezvimwe tsvina zviri panzvimbo yekunamira zvinofanirwa kubviswa zvisati zvanamira.