AWS E410NiMo -15 Stainless Steel Welding Electrode ine Yakaderera Hydrogen Sodium Coating, Arc Welding Stick

Tsanangudzo Pfupi

G207NiMo (AWS E410NiMo -15) is a martensitic Stainless steel electrode ine yakaderera hydrogen sodium coating.


Product Detail

Product Tags

Stainless Simbi WeldingElectrode

G207NiMo                                                     

GB/T E410NiMo -15

AWS E410NiMo -15

 

Tsanangudzo: G207NiMo is a martensitic Stainless steel electrode ine yakaderera hydrogen sodium coating.Shandisa DCEP (yakananga ikozvino electrode yakanaka) uye inogona kusungirirwa munzvimbo dzese.Iyo yekumusoro layer ine yakanaka anti-cavitation uye anti-jecha kupfeka zvivakwa.Iyo yekumusoro welding process iri nyore, hapana chikonzero chekupisa pamberi pekuisa, hapana kupisa kurapwa kunodiwa mushure mewelding, uye iyo yekumusoro layer inogona kugadzirwa.

Kushandisa: Inonyanya kushandiswa kugadzirisa welding ye0Cr13Ni4Mo simbi castings, kugadziriswa kwepamusoro kwehydropower kuyerera kwezvikamu mushure mekupfeka kwecavitation, uye welding yezvikamu zvezvimiro zvechinhu chimwe chete.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

S

P

≤0.06

≤1.0

≤0.90

11.0 ~ 12.5

4.0 ~ 5.0

0.40 ~ 0.70

≤0.03

≤0.04

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥760

≥15

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

3.2

4.0

5.0

Welding Current

(A)

80 ~ 120

120 ~ 160

150 ~ 190

Cherechedza:

1. Elekitirodhi inofanira kubikwa kweawa imwe panguva inenge 300 ℃ isati yaitwa welding;

2. Zvinokosha kuchenesa ngura, chikero chemafuta, mvura, uye tsvina pazvikamu zvewelding tisati tasveta.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo, uye welding consumables kwemakore anopfuura 20. Zvigadzirwa zvedu zvikuru zvinosanganisira simbi isina tsvinawelding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminium welding wires, submerged arc welding. .waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 