AWS A5.4 E310-16 Stainless Steel Welding Electrodes Welding Stick Welding Materials

Tsanangudzo Pfupi

A402 (AWS E310-16) ndeye Cr26Ni21 pure austenitic stainless steel electrode ine titanium calcium coating.


Product Detail

Product Tags

Stainless Simbi Welding Electrode

A402                                   

GB/T E310-16

AWS A5.4 E310-16

 Tsanangudzo: A402 ndeye Cr26Ni21 pure austenitic Stainless steel electrode ine titanium calcium coating.Inogona kushandiswa kune ese AC uye DC ine yakanakisa mashandiro ekushanda.Iyo simbi yakaiswa ine yakanaka oxidation kuramba pasi peyakanyanya tembiricha mamiriro e900 ~ 1100 ℃.

Chishandiso: Inoshandiswa kukwirisa mhando imwechete yesimbi inodzivirira kupisa inoshanda pasi petembiricha yakakwira, uye inogona zvakare kushandiswa kugadzira simbi dzakaomeswa dzechromium (senge Cr5Mo, Cr9Mo, Cr13 uye Cr28, nezvimwewo) nemasimbi akasiyana.

 

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

0.08 ~ 0.20

1.0 ~ 2.5

≤0.75

25.0 ~ 28.0

20.0 ~ 22.5

≤0.75

≤0.75

≤0.030

≤0.030

 

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥550

≥25

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

 

Cherechedza:

  1. Iyo electrode inofanira kubikwa kweawa imwe pakutenderera 250 ℃ isati yaitwa welding;
  2. Nekuti kudzika kwekupinda hakuna kudzika panguva ye AC welding, iyo DC magetsi inofanirwa kushandiswa zvakanyanya sezvinobvira kuwana yakadzika kupinda.uye ikozvino haifaniri kunge yakakura zvakanyanya kudzivirira kutsvuka kwetsvimbo yewelding.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 

 

 


  • Zvakapfuura:
  • Zvinotevera: