E70C-6M Carbon Steel Flux Cord Arc Welding Electrodes Flux Core Welding Wire

Tsanangudzo Pfupi

E70C-6M simbi-cored welding wire inosanganisa kushanda kwewaya dzakasimba (GMAW) nehupamhi hwekugadzirwa kwemazinga e flux-cored (FCAW) waya-yakaderera fume generation rates, yakakwirira kushanda zvakanaka, hapana slag yekuchenesa kana kubvisa-nese zvakanakira cored. waya dzine pamusoro pewaya dzakasimba-hapana "inotonhora lap" kana kushaikwa kwekusanganiswa kwepadivi, kupfapfaidza kwakachena ne75-80% argon/balance carbon dioxide, kukurumidza kufamba kumhanya kweiyo fillet size yakapihwa.


Product Detail

Product Tags

E70C-6M simbi-cored welding wire inosanganisa kushanda kwewaya dzakasimba (GMAW) nehupamhi hwekugadzirwa kwemazinga e flux-cored (FCAW) waya-yakaderera fume generation rates, yakakwirira kushanda zvakanaka, hapana slag yekuchenesa kana kubvisa-nese zvakanakira cored. waya dzine pamusoro pewaya dzakasimba-hapana "inotonhora lap" kana kushaikwa kwekusanganiswa kwepadivi, kupfapfaidza kwakachena ne75-80% argon/balance carbon dioxide, kukurumidza kufamba kumhanya kweiyo fillet size yakapihwa.E70C-6M inonyatsokodzera maapplication uko yakakwirira manganese nesilicon mazinga akakosha, senge pamberi peinorema mill scale kana mild contaminants, kana painoda kunyorova weld bead.Ichi chigadzirwa chinokunda mune zvakajairwa chinangwa chewelding, asi chakakwirira zvakaenzana mumamiriro ekudiwa kwepamusoro sepakurema kwesimbi kugadzirwa kwesimbi, basa rekuvaka, pombi welding uye welding yezvidziya zvemvura inopisa.

AWS Kirasi: E70C-6M Certification: AWS A5.18/A5.18M:2005
Alloy: E70C-6M ASME SFA A5.18

 

Welding Position: F, H, V, OH .035-1/16”
F, H 5/64”-1/8”
Zvazvino:
DCEP

 

Kusimba Simba, kpsi: 70 100% CO2
Goho Simba, kpsi: 58 100% CO2
Elongation mu2"%: 22 100% CO2

Typical Wire Chemistry as per AWS A5.18 ( single values ​​is maximum)

C Mn Si S P Ni Cr Mo V Cu  
0.12 1.75 0.90 0.03 0.03 0.50 0.20 0.30 0.08 0.50  
Typical Welding Parameters
Diameter Process Volt Amps Shielding Gasi
in (mm)
.035 (0.9) GMAW 24-35 160-250 75-95% Ar/balance Co2, 35-50cfh
.045 (1.2) GMAW 37-33 180-330 75-95% Ar/balance Co2, 35-50cfh
.052 (1.3) GMAW 25-35 220-460 75-95% Ar/balance Co2, 35-50cfh
1/16 (1.6) GMAW 26-37 240-520 75-95% Ar/balance Co2, 35-50cfh
5/64 (2) GMAW 27-36 240-550 75-95% Ar/balance Co2, 35-50cfh
3/32 (2.4) GMAW 28-36 350-550 75-95% Ar/balance Co2, 35-50cfh
7/64 (2.78) GMAW 27-34 400-600 75-95% Ar/balance Co2, 35-50cfh
1/8 (3.2) GMAW 26-32 95-145 75-95% Ar/balance Co2, 35-50cfh

 

Wenzhou Tianyu Electronic Co., Ltd yakavambwa muna 2000.welding tsvimbo, uye welding consumables kweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.