AWS E309L-15 Stainless Steel Welding tsvimbo, Stainless simbi solder Arc Welding Electrode

Tsanangudzo Pfupi

A067 (AWS E309L-15) ishoma-hydrogen sodium mhando Ultra-low kabhoni Cr23Ni13 Stainless simbi electrode.


Product Detail

Product Tags

Stainless Simbi WeldingElectrode

A067                                         

GB/T E309L-15

AWS E309L-15

Tsanangudzo: A067 imhando yakaderera-hydrogen sodium yemhando yepamusoro-yakaderera kabhoni Cr23Ni13 Stainless steel electrode.Shandisa DCEP (yakananga ikozvino electrode yakanaka) uye inogona kusungirirwa munzvimbo dzese.Iyo ine yakaderera kabhoni yemukati, saka inokwanisa kuramba intergranular corrosion inokonzerwa nekunaya kwecarbide isina zvigadzikiso senge niobium uye titanium.

Chikumbiro: Inoshandiswa kune imwecheteyo mhando yesimbi isina simbi chimiro, inoumbwa simbi uye yakakosha-yakaumbwa simbi zvikamu mukugadzira yakagadzirwa fiber, petrochemical nemimwe michina.Iyo inogona zvakare kushandiswa kukwirisa pamusoro peaya ekuchinja pamadziro emukati menyukireya reactor pressure midziyo uye welding yeshongwe yemukati zvinhu.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥520

≥25

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~ 70

80 ~ 120

130 ~ 160

160 ~ 200

 

Cherechedza:

1. Elekitirodhi inofanira kubikwa kweawa imwe panguva inenge 300 ℃ isati yaitwa welding;

2. Zvinokosha kuchenesa ngura, chikero chemafuta, mvura, uye tsvina pazvikamu zvewelding tisati tasveta.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo,uyewelding zvinodyiwakweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira simbi isina tsvinawelding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminium welding wires, submerged arc welding. .waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.