AWS E9016-B3 Heat Resistant Steel Welding Electrode R406 Wear-Resistant Welding Electrode

Tsanangudzo Pfupi

R406 (AWS E9016-B3) inonzi pearlitic heat-resistant steel electrode ine low-hydrogen potassium coating ine 2.5% Cr - 1% Mo.


Product Detail

Product Tags

Molybdenum uye Chromium Molybdenum Heat ResistantSimbi WeldingElectrode

R406                                                     

GB/T E6016-B3

AWS A5.5 E9016-B3

Tsanangudzo: R406 is pearlitic heat-resistant steel electrode ine yakaderera-hydrogen potassium coating ine 2.5% Cr - 1% Mo.Both AC uye DC inogona kushandiswa, uye inogona kusungirirwa munzvimbo dzose.Iyo weldment inofanira kunge isati yapisa kusvika 160 ~ 200 ° C isati yave nemoto.

Chikumbiro: Inoshandiswa kushivirira Cr2.5Mo pearlitic inodzivirira kupisa simbi zvimiro, senge tembiricha yepamusoro uye yakakwirira-kudzvanywa mapaipi ane tembiricha yekushanda iri pasi pe550 ° C, michina yemakemikari yekugadzira, uye petroleum inopwanya michina.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.50

2.00 ~ 2.50

0.90 ~ 1.20

≤0.030

≤0.030

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Goho simba

Mpa

Elongation

%

Impact value (J)

Normal Temp.

Guaranteed

≥590

≥490

≥15

≥47

 

Diffusion hydrogen zvemukati mesimbi yakaiswa: ≤4.0mL/100g (glycerin nzira)

 

X-ray kuongorora: Ini giredhi

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

5.0

WeldingCurrent

(A)

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Cherechedza:

1. Elekitirodhi inofanira kubikwa kweawa imwe panguva inenge 350 ℃ isati yaitwa welding;

2. Zvinokosha kuchenesa ngura, chikero chemafuta, mvura, uye tsvina pazvikamu zvewelding tisati tasveta.

 