R306 (AWS E8016-B2) inonzi pearlitic heat-resistant steel electrode ine low-hydrogen potassium coating ine 1% Cr - 0.5% Mo.


Product Detail

Product Tags

Molybdenum uye Chromium Molybdenum Heat Resistant SimbiWeldingElectrode

R306                                                     

GB/T E5516-B2

AWS A5.5 E8016-B2

Tsanangudzo: R306 inonzi pearlitic heat-resistant steel electrode ine yakaderera-hydrogen potassium coating ine 1% Cr - 0.5% Mo. Zvose AC uye DC zvinogona kushandiswa, uye zvinogona kusungirirwa munzvimbo dzose.Iyo weldment inofanira kunge isati yapisa kusvika 160 ~ 250 ° C isati yave nemoto.

Chikumbiro: Inoshandiswa pakunama Cr 1% - Mo 0.5% simbi inodzivirira kupisa iyo tembiricha yekushanda iri pasi pe520 ℃, senge pombi dzebhailer, midziyo yekumanikidza, vaporizer uye petroleum yekunatsa michina, nezvimwe.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.60

0.80 ~ 1.50

0.40 ~ 0.65

≤0.030

≤0.030

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Goho simba

Mpa

Elongation

%

Impact value (J)

Normal Temp.

Guaranteed

≥540

≥440

≥17

≥47

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

60 ~ 90

90 ~ 130

140 ~ 180

180 ~ 210

 

Cherechedza:

1. Elekitirodhi inofanira kubikwa kweawa imwe panguva inenge 350 ℃ isati yaitwa welding;

2. Zvinokosha kuchenesa ngura, chikero chemafuta, mvura, uye tsvina pazvikamu zvewelding tisati tasveta.

 

 