A032Mo (AWS E317L-16) is an ultra-low carbon Cr19Ni13Mo3 Stainless steel electrode ine titanium calcium coating.


Product Detail

Product Tags

Stainless Simbi WeldingElectrode

A032Mo                                            

GB/T E317L-16

AWS E317L-16

Tsanangudzo: A032Mo is an ultra-low carbon Cr19Ni13Mo3 Stainless steel electrode ine titanium calcium coating.Inogona kushandiswa kune ese AC uye DC ine yakanaka maitiro ekuita.Iyo corrosion resistance kune sulfuric acid, sulfurous acid uye organic acid iri nani pane yeE316L.

Chishandiso: Inoshandiswa kukwirisa mhando imwechete yesimbi isina tsvina senge AISI317 uye 317L simbi, uye inokodzerawo welding uye nepamusoro-soro-inodzivirira mirairi yesimbi inoumbwa uye yakakosha-yakaita simbi.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

3.0 ~ 4.0

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥520

≥25

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 220

 

Cherechedza:

1. Elekitirodhi inofanira kubikwa kweawa imwe panguva inenge 250 ℃ isati yaitwa welding;

2. Zvinokosha kuchenesa ngura, chikero chemafuta, mvura, uye tsvina pazvikamu zvewelding tisati tasveta.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo,uyewelding zvinodyiwakweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.


  • Zvakapfuura:
  • Zvinotevera: