AWS E312-16 Kukwesha Simbi Isina KusimbaElectrodeTsvimbo
Solder/Filler Rod rudzi rwe electrode yesimbi ine zvikamu zviviri ine lime-titania coating. Nekuda kwe40% ferrite iri musimbi yakachengetwa, solder ine resistance yakanaka kwazvo yekupwanya. Solder ine welding performance yakanaka kwazvo. Filler rod inoshandiswa pakuwelda simbi ine kabhoni yakawanda, simbi yezvishandiso, simbi inodziya zvakanyanya, simbi yezvombo, simbi dzakasiyana, nezvimwewo. Soldering rod ine welding performance yakanaka kwazvo, resistance yakanaka kwazvo yekupwanya, uye dual-phase steel electrode ine lime-titania type coating.
Nhamba yeModhero: E312-16 electrode yesimbi isina ngura
Zvinhu: Simbi Isina Chinovhara
Kureba: 300mm-500mm
Dhayamita: 2.0mm, 2.5mm, 3.2mm, 4.0mm
Kushandiswa: Simba guru resimbi yemadota uye simbi yesimbi yebhora
| Electrode yeSimbi Isina Mapato Maviri AWS E312-16 GB E312-16 | |
| Nhanganyaya: A1002 imhando yeelectrode yesimbi ine zvikamu zviviri ine lime-titania coating. Nekuda kwe40% ferrite iri musimbi yakachengetwa, ine simba rakanaka rekudzivirira kutsemuka. Inoshanda zvakanaka pakuwelda. | |
| Mashandisirwo: Inoshandiswa pakusondera simbi ine kabhoni yakawanda, simbi yezvishandiso, simbi inodziya zvakanyanya, simbi yezvombo, simbi yakasiyana, nezvimwewo. |
Kuumbwa kweMakemikari eSimbi Yakachengetwa (%)
| Kuumbwa kweMakemikari | C | Mn | Si | S | P | Ni | Cr |
| Kukosha kweVimbiso | ≤0.15 | 0.5~2.5 | ≤0.90 | ≤0.030 | ≤0.040 | 8.0~10.5 | 28.0~32.0 |
Zvimiro zveMechanical zveSimbi Yakachengetwa
| Chinhu Chekuyedza | Rm(MPa) | A(%) |
| Kukosha kweVimbiso | ≥660 | ≥22 |
Referensi yeKushandiswa Kwemagetsi (AC, DC+)
| Dhayamita yeElectrode (mm) | φ2.5 | φ3.2 | φ4.0 | φ5.0 |
| Kuwedera Kwemagetsi (A) | 50~80 | 80~110 | 110~160 | 160~220 |
Mirayiridzo:
1. Maelectrode anofanira kubikwa pasi pe 250°C kweawa imwe chete asati abatanidza.
2. Direct current inofanira kushandiswa zviri nani uye current haifanirwe kunge yakasimba zvakanyanya.
Kurongedza & Kutumira
Ruzivo rweKurongedza: 5kgs/bhokisi, 20kgs/bhokisi
Ruzivo rwekutumira: 20-25days