Tyue Brand AWS ENiCrMo-4 Nickel uye Nickel Yakavakirwa Alloy Welding Electrode, Best Arc Welding Rods, Welding Supplier

Tsanangudzo Pfupi

Ni327-4 (ENiCrMo-4) is nickel-based electrode ine low-hydrogen sodium coating.Shandisa DCEP (yakananga ikozvino electrode yakanaka).


Product Detail

Product Tags

Nickel uye Nickel Alloy Welding Electrode

Ni327-4                                                     

GB/T ENi6276

AWS A5.11 ENCrMo-4

 

Tsanangudzo: Ni327-4 is nickel-based electrode ine yakaderera-hydrogen sodium coating.Shandisa DCEP (yakananga ikozvino electrodepositive).Iyo ine yakanakisa welding performance ine yakagadzikana arc combustion, shoma spatter, nyore kubvisa slag,

uye weld yakanaka.Iyo mechanical properties yesimbi yakaiswa yakagadzikana.

 

Chikumbiro: Inoshandiswa kukwenenzvera yakaderera-kabhoni nickel-chromium-molybdenum alloys, seHastelloy C276, ASTM B574, B575, B619, B622, B626, uye inogona zvakare kushandiswa kugadzira masimbi akasiyana nemamwe nickel-based alloys.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

≤0.02

≤1.0

≤0.2

14.5 ~ 16.5

≥50.0

15.0 ~ 17.0

W

Co

Fe

S

P

Zvimwe

3.0 ~ 4.5

≤2.5

4.0 ~ 7.0

≤0.015

≤0.020

≤0.5

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Goho simba

Mpa

Elongation

%

Guaranteed

≥690

≥400

≥22

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

Welding ikozvino

(A)

60 ~ 90

70 ~ 110

90 ~ 150

 

Cherechedza:

1. Elekitirodhi inofanira kubikwa kweawa imwe panguva inenge 300 ℃ isati yaitwa welding.Edza kushandisa arc pfupi kuti weld;

2. Zvakakosha kuchenesa dzine ngura, oiri, mvura, uye tsvina pazvikamu zvinonamatwa tisati tapisa.

3. Edza kushandisa simba remutsara mudiki paunenge uchitsvaira, multi-layer uye multi-pass welding.

 