ER1100 A5.10 Aluminium Weding Wire Mig Rods and Electrodes

Tsananguro pfupi:

ER1100 inodzivirira zvakanyanya kurwiswa nemakemikari uye mamiriro ekunze. Isimbi yakapfava uye inogadzirwa zvakanaka uye inoshandiswa zvakanyanya muzvigadzirwa zve thin gauge uye foil.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

ER1100 A5.10, ALUMINUM UYE ALUMINUM ALLOY Maelectrodes neTsvimbo

ER1100 inodzivirira zvakanyanya kurwiswa nemakemikari uye mamiriro ekunze. Isimbi yakapfava uye inogadzirwa zvakanaka uye inoshandiswa zvakanyanya muzvigadzirwa zve thin gauge uye foil. Ine hunhu hwakanaka hwekunyorovesa uye inoshandiswawo sesimbi yekuzadza yekubatanidza. Hunhu hunodiwa hwesimbi iyi kupenya kwakajeka kunowanikwa nekushandisa anodizing.

Mashandisirwo Akajairika: kuchinjana kupisa; michina yekubata chikafu; rivets; tai waya; simbi

Kirasi yeAWS: ER1100 Chitupa: AWS A5.10/ A5.10M:1999
Chiwanikwa: ER1100 AWS/ASME SFA A5.10

 

Nzvimbo Yekushongedza:
F, V, OH, H
Zvazvino:
DCEP-GMAW
AC-GTAW

 

Zvimiro Zvakajairika (sezvakasungirirwa)

Kufambisa: 59% IACS (-12)
Simba reKusimba, kpsi: 13
Ruvara: Gireyi
Nzvimbo Yokunyunguduka 1215⁰F Kusimba 1090⁰F Kuwanda kwevanhu 0.098 lbs/cu Mukati.

Kemikari yeWaya Yakajairika zvichienderana neAWS A5.10 (hunhu humwe chete ndihwo hwakanyanya)

Si + Fe Cu Mn Zn Zvimwe Al  
0.95 0.05-0.20 0.05 0.10 0.15 99.0 maminiti  
Zvakajairika Zvekushongedza Zvimiro
Dhayamita Maitiro Volt Maampisi GESI
in (mm)
.030 (.8) GMAW 15-24 60-175 Argon (cfh)
.035 (.9) GMAW 15-27 70-185 Argon (cfh)
3/64” (1.2) GMAW 20-29 125-260 Argon (cfh)
1/16” (1.6) GMAW 24-30 170-300 Argon (cfh)
3/32” (2.4) GMAW 26-31 275-400 Argon (cfh)
Dhayamita Maitiro Volt Maampisi GESI
in (mm)
1/16” (1.6) GTAW 15 60-80 Argon (cfh)
3/32” (2.4) GTAW 15 125-160 Argon (cfh)
1/8” (3.2) GTAW 15 190-220 Argon (cfh)
5/32” (4.0) GTAW 15 200-300 Argon (cfh)
3/16” (4.8) GTAW 15-20 330-380 Argon (cfh)

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave tichigadzira maerekitironi ekuwelda, tsvimbo dzekuwelda, uye zvinhu zvinoshandiswa pakuwelda kweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira maelectrode esimbi isina ngura, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni & cobalt, mawaya esimbi yekabhoni & low alloy, waya dzesimbi yekabhoni & low alloy, waya dzesimbi yekabhoni, waya dzesimbi yekabhoni, waya dzakavharirwa negesi, waya dzesimbi yekabhoni ...

 

 