Tsvimbo yeWelding yeSimbi Isina Stainless E308L-17

Tsananguro pfupi:

E308L-17 Yesimbi Isina Kugayiwa Electrode Welding Rod (Low C, 18%Cr- 8%Ni)


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

E308L-17 Yesimbi Isina Kugayiwa Electrode Welding Rod (Low C, 18%Cr- 8%Ni)

Kupatsanura

EN IS03581-A:2016: E 19 9 L R 12

EN IS03581-B:2016: ES308L-17

AWS A5.4-2014: E308L-17

JISZ 3221-2013: ES308L-17

Tsananguro

-Kufukidza kwacho kunoitwa nerudzi rwe lime titania yekunamira simbi isingatsvi ye18%Cr-8%Ni. (AISI 301, 302, 304, 308)

-Kushanda zvakanaka kwewelding nekuda kwehuwandu hwakawanda hwekuisa simbi.

-Bvisa Mvura, ngura, mafuta nezvimwe zvinhu zvisina kunaka kubva mumugero usati wabatanidza.

-Kushandiswa kwakanaka nekushandisa magetsi zvakananga.

-Kudziisa moto usati watanga hazvidiwi kazhinji.

-Chengeta electrode pa 250~350°C kwemaminitsi 30~60 usati washandisa.

Kuumbwa kweMakemikari Simbi Yakachengetwa (%)
C Mn Si Cr Ni S P Mo Cu Fn
0.03 0.65 0.73 18.95 9.82 0.012 0.028 0.21 0.30 6.4

 

Saizi & Zvinokurudzirwa Zvemazuva Ano (AC kana DC)
Dhayamita yetsvimbo yekuwedera
(mm)
2.5 3.2 4.0 5.0
welding current
(A)
55-80 90-130 110-150 140-180

Hunhu hweMashandisirwo:

Arc yakasimba kwazvo.

Kubviswa kwakanaka kwetsvina.

Kupinda mukati hakuna kudzika.

Kudzivirira kupisa nekuora zvakanaka.

Kudzivirira kutsemuka kwakanaka.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave tichigadzira maerekitironi ekuwelda, tsvimbo dzekuwelda, uye zvinhu zvinoshandiswa pakuwelda kwemakore makumi maviri nemaviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira maelectrode esimbi isina ngura, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni & cobalt, mawaya esimbi yekabhoni & low alloy, waya dzesimbi yekabhoni & low alloy, waya dzesimbi yekabhoni, waya dzakavharirwa negesi, waya dzesimbi yekabhoni, welding yesimbi yekabhoni, welding yesimbi yekabhoni, waya dzesimbi dzakadzivirirwa nemagetsi, waya dzesimbi yekabhoni, welding yesimbi yekabhoni, waya dzesimbi dze ....


  • Yakapfuura: