AWS E8018-B2 Chromium Molybdenum Welding Steel Resistant Heat Resistant Electrode R306Fe Stick Electrodes Welding Consumables

Tsananguro pfupi:

R306Fe (AWS E8018-B2) ielectrode yesimbi inodzivirira kupisa ine hupfu hwesimbi uye hydrogen potassium coating ine 1% Cr - 0.5% Mo.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Molybdenum neChromium Molybdenum Molybdenum Electrode Yekushongedza Simbi Inodzivirira Kupisa

R306Fe                                                     

GB/T E5518-B2

AWS A5.5 E8018-B2

Tsananguro: R306Fe ielectrode yesimbi inodzivirira kupisa ine hupfu hwesimbi uye hydrogen potassium coating yakaderera ine 1% Cr - 0.5% Mo. AC neDC zvese zvinogona kushandiswa, uye zvinogona kusungirirwa munzvimbo dzese nekushanda kwenguva pfupi kwearc. Kudziisa kweweldment uye tembiricha yepakati pezvikamu ndeye 160 ~ 250 °C panguva yekusungirirwa.

Mashandisirwo: Inoshandiswa pakunamira simbi ye1%Cr – 0.5%Mo ine pearlitic inodzivirira kupisa (yakadai se15CrMo), yakaita semapaipi ekupisa pamusoro pebhoyira ane tembiricha yekushanda iri pasi pe550°C, mapaipi emhepo uye midziyo yekumanikidza ine tembiricha yekushanda iri pasi pe520°C, nezvimwewo. Inogona kushandiswa pakunamira simbi ye30CrMnSi.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.50

1.00 ~ 1.50

0.40 ~ 0.65

≤0.030

≤0.030

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Kukosha kwemhedzisiro (J)

Kupisa Kwakajairika.

Yakavimbiswa

≥540

≥440

≥47

≥27

Yakaedzwa

550 ~ 640

≥450

20 ~ 28

105 ~ 150

 

Kupararira kwehydrogen musimbi yakachengetwa: ≤6.0mL/100g (nzira yeglycerin)

 

Kuongororwa kweX-ray: Giredhi I

 

Inokurudzirwa yemagetsi:

Dhayamita yetsvimbo

(mm)

3.2

4.0

5.0

Welding Current

(A)

100 ~ 130

140 ~ 180

180 ~ 210

 

Cherechedza:

1. Electrode inofanira kubikwa kweawa imwe chete pakupisa kwe350℃ isati yashandiswa pakunamira;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira.