W707Ni Welding Yesimbi Yekupisa Kwakaderera Electrode Yekushongedza Inonamira Yehydrogen Yakaderera Vatengesi

Tsananguro pfupi:

W707Ni ielectrode yesimbi inodziya zvishoma ine Ni mu hydrogen sodium coating ine hydrogen sodium shoma.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Simbi Inodziya ZvishomaKushongedzaElectrode

W707Ni                                                     

GB/T E5515-C1

Tsananguro: W707Ni ielectrode yesimbi ine tembiricha yakaderera ine Ni mu hydrogen sodium coating ine hydrogen shoma. Shandisa DCEP (direct current electrode positive) uye inogona kusungirirwa munzvimbo dzese. Simbi yakachengetwa ichiri yakasimba pa -70°C.

Kushandiswa: Kunoshandiswa pakusondera simbi ine tembiricha yakaderera senge 2.5Ni.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Si

Ni

S

P

≤0.12

≤1.25

≤0.60

2.00 ~ 2.75

≤0.020

≤0.025

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Kukosha kwemhedzisiro (J)

-70℃

Yakavimbiswa

≥540

≥440

≥17

≥27

 

Kupararira kwehydrogen musimbi yakachengetwa: ≤6.0mL/100g (nzira yeglycerin) kana ≤10mL/100g (nzira yemercury kana gas chromatography)

Kuongororwa kweX-ray: Giredhi I

 

Inokurudzirwa yemagetsi:

(mm)

Dhayamita yetsvimbo

2.0

2.5

3.2

4.0

5.0

(A)

Welding Current

40 ~ 70

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 Cherechedza:

  1. Electrode inofanira kubikwa kweawa imwe pa350℃ isati yashandiswa pakunamira;
  2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira;
  3. Edza kushandisa simba diki pakusanganisa simbi, kusanganisa simbi dzakawanda uye kusanganisa simbi dzakawanda.

 


  • Yakapfuura:
  • Zvinotevera: