AWS E7015-C2L Yakaderera Tembiricha Simbi Welding Electrode W107 Welding Tsvimbo Yakaderera Hydrogen Electrode ARC Stick Welding

Tsanangudzo Pfupi

W107 (AWS E7015-C2L) isimbi yakadzika-tembiricha electrode ine yakaderera-hydrogen sodium coating..Shandisa DCEP (yakananga ikozvino electrode yakanaka) uye inogona kusungirirwa munzvimbo dzese.Simbi yakaiswa ichiri iine kunaka kwesimba kusimba pa -100°C.


Product Detail

Product Tags

Yakaderera Tembiricha Simbi Welding Electrode

W107                                                     

GB/T E5015-C2L

AWS A5.5 E7015-C2L 

Tsanangudzo: W107 isimbi yakadzika-tembiricha electrode ine yakaderera-hydrogen sodium coating.Shandisa DCEP (yakananga ikozvino electrode yakanaka) uye inogona kusungirirwa munzvimbo dzese.Simbi yakaiswa ichiri iine kunaka kwesimba kusimba pa -100°C. 

Chikumbiro: Inoshandiswa pakushongedza yakaderera tembiricha simbi senge 3.5Ni.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Ni

S

P

≤0.05

≤1.25

≤0.60

3.00 ~ 3.75

≤0.020

≤0.025

 

Mechanical zvimiro zve weld simbi:

 

Test chinhu

 

Kusimba simba

Mpa

 

Goho simba

Mpa

Elongation%

Impact value (J) -100℃

 

Guaranteed

≥490

≥390

≥22

≥27

 

Diffusion hydrogen yemukati mesimbi yakaiswa: ≤4.0mL/100g (glycerin nzira) kana ≤7.0mL/100g (mercury kana gasi chromatography nzira)

 

X-ray kuongorora: Ini giredhi

 

Yazvino inokurudzirwa:

(mm)

Tsvimbo dhayamita

2.0

2.5

3.2

4.0

5.0

(A)

Welding Current

40 ~ 70

70 ~ 90

90 ~ 130

140 ~ 180

180 ~ 240

 

 

Cherechedza:

  1. Iyo electrode inofanira kubikwa kweawa imwe pa350 ℃ isati yaitwa welding;
  2. Zvinokosha kuchenesa ngura, chikero chemafuta, mvura, uye tsvina pazvikamu zvewelding tisati taputirwa;
  3. Edza kushandisa simba remutsara mudiki paunenge uchitsvaira, multi-layer uye multi-pass welding.

 