TYUE E6013(J421X) CARBON STEEL ELECTRODE

Tsananguro pfupi:

AWS A5.1 E6013(J421) ielectrode yerudzi rwerutile.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Kupatsanura:

ISO 2560-A-E35 0 RA 12

AWS A5.1: E6013

GB/T 5117 E4313

Hunhu:

AWS A5.1 E6013(J421X) ielectrode yerudzi rwe rutile. Inogona kusungirirwa simba reAC neDC uye inogona kushandiswa munzvimbo dzese. Ine mashandiro akanaka ekushongedza se arc yakagadzikana, smatter diki, nyore kubvisa slag uye kugona kudzoreredza simba nezvimwewo. Electrode yeRutile-cellulosic ine kugona kwakanaka kwekushongedza munzvimbo dzese kusanganisira vertical down. Kugona kwakanaka kwepakati uye kurova arc. Yekubatanidza tack uye kutakura mutoro. Chinangwa chikuru cheindasitiri nekutengeserana, kuunganidza uye kushongedza shopu.

Kuumbwa kweMakemikariYesimbi Yese Yakasungirirwa:(%)
Kuumbwa kweMakemikari C Mn Si S P Ni Cr Mo V
Zvinodiwa ≤0.10 0.32-0.55 ≤0.30 ≤0.030 ≤0.035 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Mhedzisiro Yakajairika 0.08 0.37 0.18 0.020 0.025 0.030 0.035 0.005 0.004
Zvimiro zveMechanical zveSimbi Yakachengetwa
Chinhu Chekuyedza Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Zvinodiwa 440-560 ≥355 ≥22 ≥47
Mhedzisiro Yakajairika 500 430 27 80
Referensi Yazvino (DC)
Dhayamita φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage 40 ~ 70 50 ~ 90 80~ 130 150 ~ 210 180 ~ 240

Nzvimbo Yekushongedza:

PA, PB, PC, PD, PE, PF

Kuongorora X-Ray Radiographic:

DhigiriiⅡ

Kuchenjerera:

Kazhinji, usaita'Hamufanirwe kuomesa electrode zvakare musati maibatanidza. Kana yakanganiswa neunyoro, inofanira kuomesazve pa 150℃-170℃kweawa 0.5-1.