GB/T EZNiCu-1 (Z508) Cast Iron Welding Electrode Nickel-Copper Alloy (Monel) Core uye Graphitized Coating

Tsanangudzo Pfupi

GB/T EZNiCu-1 (Z508) inonzi cast iron welding electrode ine nickel-copper alloy (Monel) core uye graphitized coating.


Product Detail

Product Tags

Cast Iron WeldingElectrode

Z508                                                     

GB/T EZNiCu-1

Tsanangudzo: Z508 is cast iron welding electrode ine nickel-copper alloy (Monel) core uye graphitized coating.AC uye DC mbiri-chinangwa, yakagadzikana arc, iri nyore kushanda.Kugadzirwa kwayo uye kuita kwekucheka kuri padyo neZ308, asi nekuda kwekukura kukuru kwesimbi yakaiswa, kutsemuka kuramba kwakashata.Simba remajoini akasungwa rakaderera, saka haakodzeri welding yezvikamu zvakamanikidzwa.

Kushandisa: Inoshandiswa kugadzira welding yegrey iron castings iyo isingade simba rakawanda.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Si

Mn

Fe

S

Ni

Cu

Vamwe

0.35 ~ 0.55

≤0.75

≤2.3

3.0 ~ 6.0

≤0.025

60 ~ 70

25 ~ 35

≤1.0

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

3.2

4.0

5.0

Welding ikozvino

(A)

90 ~ 110

120 ~ 150

160 ~ 190

 

Cherechedza:

1. Elekitirodhi inofanira kubikwa kweawa imwe inenge 150 ℃ isati yaitwa welding;

2. Paunenge uchitsvaira, zvinokurudzirwa kushandisa nzira yakamanikana, uye kureba kweweld imwe neimwe haifaniri kudarika 50mm.Pakarepo nyundo weld nenyundo diki kuti ubvise kushushikana munzvimbo yekugadzira weld uye kudzivirira kutsemuka mushure mekuputika.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzira maelectrode e welding, welding rods, uye.welding inodyiwas kweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 