AWS EN-C1 (Z308) Nickel Yakachena Kukandira Simbi Inoputira Electrode Nickel 99 Welding Tsvimbo Arc Tsvimbo Electrodes Ni99

Tsanangudzo Pfupi

AWS ENi-C1 (Z308) isimbi yakakandwa electrode ine yakaderera kabhoni simbi core uye yakasimba graphitized coating.


Product Detail

Product Tags

Kanda Iron Welding Electrode

Z308                                                     

GB/T EZNi-1

AWS A5.15 EN-C1

Tsanangudzo: Z208 isimbi yakakandwa electrode ine yakaderera kabhoni simbi core uye yakasimba graphitized coating.Inogona kushandiswa kune ese AC uye DC.Iyo weld inogona kuita grey cast iron kana ikatonhodzwa zvishoma nezvishoma, asi kusamira kwayo pakutsemuka hakuna kunaka.

Kushandisa: Inoshandiswa kugadzirisa kukanganisa mune grey iron castings.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Si

Mn

S

Ni

Fe

Vamwe

≤2.0

≤2.5

≤1.0

≤0.03

≥90

≤8.0

≤1.0

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.5

3.2

4.0

Welding ikozvino

(A)

65 ~ 90

90 ~ 110

120 ~ 150

 

Cherechedza:

1. Elekitirodhi inofanira kubikwa kweawa imwe inenge 150 ℃ isati yaitwa welding;

2. Kushungurudzika munzvimbo yekugadzira welding kunogona kubviswa nekurova weld kuti usatsemuka.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave mushishi mukugadzira maelectrode ewelding, welding rods, uye welding consumables kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira Stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, Stainless steel welding wires, gas-shielded flux cored wires, aluminium welding waya, yakanyura arc welding.waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 